Hong Huiping, Cheng Man, Kang Yonglin , Feng Changtao, Chen Xiqiang. Finite Element Analysis of Influence Parameters on Tension of
Φ200 mm H11 Steel Round Bar for Mandrel during Hot
Continuous Rolling[J]. Special Steel, 2006, 27(3): 5-7.
1 MSC. MARC 2005, User Manual 2005, MSC. Software Coiporation.
2洪慧平,康永林,椭圆孔型轧制合金钢方坯三维弹塑性有限元 模拟,北京科技大学学报,2003,25(2):171
3 Huiping 而咯,Yoiglin Kang, Changtao Feng. Three-Dimensiwial Thermo-Mechanical Coupled FEM Simulation for Hot Continuous Rolling of Large-Diameter Mandrel Bar. Journal of Materials Science and Technology,2003,19(Suppl.):228