φ1200 mm×380 mm 双辊薄带连铸机布流的物理模拟

Chen Yuanqing,Wen Guanghua,Zhu Mingmei , Ding Peidao   

  1. College of Materials Science and Engineering,Chongqing University,Chongqing 400044
  • Received:2006-01-24 Online:2006-08-01 Published:2023-03-17

Physical Modeling of Feeding Liquid Steel into Bath of a φ1200 mm×380 mm Twin Roll Thin Strip Concaster

陈远清,文光华, 祝明妹, 丁培道   

  1. 重庆大学材料科学与工程学院,重庆400044

  • 作者简介:陈远清(1981-),男,硕士研究生,新型连铸及相关方向。

Abstract: Simulation of liquid steel feeding system of pool in a twin roll 2~3 mm thin strip concaster with roll diame- ter 1200 mm,wide 380 mm and pool depth 460 mm at Nanchang Steel and evaluation of nozzle structure has been carried out by using 1:2.4 ratio dynamic physical model.The nozzle size structure was optimized by orthogonal experiment. The results showed that as nozzle up and down inclination is O,both sides deviation angle 60° and side hole dimension 18 mm×11 mm,the comprehensive properties of nozle were optimum and can meet the requirement of feeding liquid steel into bath.

摘要: 采用1:2.4缩小动态物理模型,对南钢辊径1 200 mm、辊宽380 mm、液面深度460 mm的双辊2- 3 mm薄带连铸机熔池布流进行模拟和水口结构进行了评估。并采用正交设计试验,对水口结构尺寸进行了优化。结果表明,水口上下倾角为0、左右偏角60°、侧孔面积为18 mm×11 mm时,水口的综合性能最佳,能满足熔池布流的要求。

关键词: 双辊薄带连铸, 浸人式水口, 熔池布流, 模拟