Finite Element Analysis on Rolling Load Parameters of Hot Continuous Mandrel Rolling of T91 Steel Seamless Tube

Hong Huiping1, Zhao Zhiyi1 , Kang Yonglin1 , Yu Yong2, Zhou Xiaolan2, Pan Feng2   

  1. 1 School of Materials Science and Engineering, University of Science and Technology, Beijing 100083 ;
    2 Steel Tube Subcompany, Baoshan Iron and Steel, Shanghai 201900
  • Received:2006-03-20 Online:2006-10-01 Published:2006-10-01

T91钢热连轧管过程力学参数的有限元分析

洪慧平1,  赵志毅1,  康永林1,  余勇2,  周晓岚2, 潘峰2   

  1. 1北京科技大学材料科学与工程学院,北京100083;
    2宝山钢铁股份有限公司钢管分公司,上海201900
  • 作者简介:洪慧平(1963-),男,博士,副教授,从事材料成形过程模 拟仿真与计算机辅助工程的教学与科研工作。

Abstract: The 8- stand floating mandrel continuous rolling process of Φ169 mm x6 mm T91 steel seamless tube has been simulated and analyzed by 3- dimensional thermo-mechanical coupled FEM to get distribution of equivalent stress of across section at exit of each pass, as well as change characteristics of rolling force, mandrel force and torque. It is proposed that increasing rolling force at first 3 stands and decreasing rolling load of 4th stand lead to reasonable distribution of rolling force parameters of continuous rolling process

摘要: 应用三维有限元模拟仿真技术,对Φ169 mmx6 mm T91无缝钢管8机架浮动芯棒连轧管过程, 进行有限元模拟与仿真分析,获得各机架横断面等效应力分布以及轧制力、芯棒力和力距的变化特点。提岀 增加前3机架轧制力,降低第4机架轧制负荷,使连轧管过程轧制力参数合理分布

关键词: T91钢, 无缝钢管, , 浮动芯棒, , 连轧过程, , 轧制力, 有限元模拟