Numerical Simulation on Oxygen Stream Field of Coherent Jet Oxygen Lance and Application to a 70 t Arc Furnace

Zhang Gui¹,Zhu Rong',Han Lihui',Zhu Changfu',Tan Zhiliang²,Liu Changchun²   

  1. 1 School of Metallurgy and Ecological Engineering,University of Science and Technology,Beijing 100083;
    2 Ezhou Steel Co,Wuhan Iron and Steel Group,Ezhou 436000
  • Received:2006-04-15 Online:2006-10-01 Published:2023-04-21
  • About author:张 贵(1981-),女,研究生,从事电弧炉用氧技术的数 值模拟研究。

70 t 电弧炉炼钢集束射流氧枪流场的数值模拟及应用

张 贵1, 朱 荣1, 韩丽辉1, 朱长富1, 谈知良2, 刘长春2   

  1. 1北京科技大学冶金与生态工程学院,北京100083;2武钢集团鄂钢公司,鄂州436000

Abstract: Numerical simulation and cold status test of jet flow of coherent jet oxygen lance and common oxygen lance for arc furnace steel making have been carried out by CFX5.7.1 Software. Results showed that the jet flow length,concentration and anti-attenuation of coherent jet oxygen lance were better than that of common oxygen lance. The application to a 70 t Consteel arc furnace at Ezhou Steel indicated that after using coherent jet oxygen lance,the electric power consumption decreased to about 219 kWh/t from 338 kWh/t,the electrode consumption was no-change (1.86 kg/t)and the oxygen consumption increased to 60.3 m³/t from original 51.6 m³/t.

摘要: 用CFX5.7.1 软件对电弧炉炼钢用集束射流氧枪和普通氧枪的射流特征进行了数值模拟和冷态试验。结果表明,集束射流氧枪比普通超音速氧枪射流长,射流集中、衰减慢。在鄂钢70 t Consteel电弧炉 上应用表明,使用集束氧枪后平均电耗由338 kWh/t降低到219 kWh/t,电极消耗未变,为1.86 kg/t,氧耗由 51.6 m³/t提高到60.3 m³/t。