Distribution of Inclusion Size in Surface Layer of IF Steel Slab under Unsteady Casting

Zhang Qiaoying,Wang  Litao,Wang  Xinhua,Wang  Wanjun, Li  Hong   

  1. 1 School of Metallurgy and Ecological Engineering,University of Science and Technology,Beijing 100083;
    2 Technology Research Institute,Capital Iron and Steel Group Corp,Beijing 100043
  • Received:2006-03-22 Online:2006-10-01 Published:2006-10-01

非稳态浇铸时IF钢铸坯表层夹杂物粒径的分布

张乔英,王立涛 ,王新华,王万军,李  宏   

  1. 1北京科技大学冶金与生态学院,北京100083;
    2首钢技术研究院,北京100043
  • 作者简介:张乔英(1976-),女,博士研究生,从事钢质量和冶金过程 数值模拟研究

Abstract: The distribution of size and frequency of inclusion in samples of surface layer of IF steel 1150 mm× 230 mm casting slab with unsteady casting speed(1.4 m/min to 0.6 m/min and 0.6 m/min to1.4 m/min)has been studied by Original Position Analysis System(OPA- 100). The results show that the distribution rule of size and frequency of inclusion basically accords with first-order exponential decay curves. The expressions of inclusion size x (μm) and frequency y is y=Al ·exp(-x/tl)+y0;A1,tl and yO are constant,R is related coefficient(R²> 0.97).

摘要: 用原位统计分布分析仪(OPA-100)研究了拉速变化时(1.4 m/min 至0.6 m/min,0.6 m/min 至 1.4 m/min)IF钢1150 mm×230 mm铸坯表层试样夹杂物粒径和频数的分布。结果表明,夹杂物粒径与其频 数分布规律基本符合一阶指数衰减曲线,夹杂物粒径x(μm) 与频数 y 的拟合公式为 y = A1 ·exp (-x/tl)+y0; 式中A1,t1,y0为常数;R 为相关系数(R²>0.97)