[1] |
Liu Junkai, Yu Yipeng, Zhang Jinglin, Zhang Jiansheng, Zhang Jianfu.
The Influence of Deformation and Heating Temperature on the Impact Toughness of 2205 Duplex Stainless Steel
[J]. Special Steel, 2024, 45(6): 69-72.
|
[2] |
Peng Feng, Li Xu, Li Bopeng, Zhang Yue, Wang Zhanzhong, Guo Shibei.
Development of 10.9 Grade 32CrB4 Quenched and Tempered Round Steel for Fasteners
[J]. Special Steel, 2024, 45(6): 8-11.
|
[3] |
Zhao Jiawei, Tian Jialong, Yang Ping, Zhan Dongping, Jiang Zhouhua.
Effect of Dual-aging Process on Microstructure and Properties of Co-precipitation Hardening Ultra-high Strength Steel
[J]. Special Steel, 2024, 45(6): 88-94.
|
[4] |
Zhao Bo, Wang Shanbao, Xie Degang, Yuan Qin, Ai Fangfang, Wang Xixiang, Guo Jinmei.
Microstructure and Properties of Seamless Steel Pipe Gr.6 after Rolling and Normalizing
[J]. Special Steel, 2024, 45(6): 102-107.
|
[5] |
Zhao Jiqing, Wan Wuxia, Li Zaoyu, Du Liqing.
Composition-Structure-Properties and Process Comprehensive Control Technology of 125ksi Super Martensitic Oil Well Pipe Material
[J]. Special Steel, 2024, 45(5): 40-46.
|
[6] |
Tang Yuanshou, Zhang Shiqing, Li Fang, He Qinsheng, Zhao Zhen, Wang Hong, Zou Xingzheng, Wang Jianqiao, Huang Yali.
Effect of Quenching Temperature on Mechanical Properties of M6C Reinforced 2 200 MPa Ultra-high Strength Steel
[J]. Special Steel, 2024, 45(5): 108-112.
|
[7] |
Wang Shaobing, Sun Wenqiang, Wang Man, Zhou Zhu, Liu Zhengdong, Zhong Qiang.
The Effect of Nb on Microstructure and Properties of GH4169 Alloy Pipe
[J]. Special Steel, 2024, 45(5): 34-39.
|
[8] |
Wang Shucai, Guo Jing, Wu Zhilong, Han Kui, Zhao Yue, Chen Xiuqiang.
Low-cost Non-vacuum Induction Furnace Smelting of High Molybdenum Content of Nickel-base Alloy
[J]. Special Steel, 2024, 45(5): 72-75.
|
[9] |
Li Qing.
Effect of Solid Solution Temperature on Microstructure and Tensile Properties of GH4163 Alloy
[J]. Special Steel, 2024, 45(5): 97-101.
|
[10] |
Yang Zhihao, Wang Linlin, Liang Tian, Jia Dongxiao, Ma Yingche, Wang Ping.
Effect of Rare Earth Gd on Thermal Deformation Behavior of Ni-Cr-Mo Alloys
[J]. Special Steel, 2024, 45(5): 8-18.
|
[11] |
Li Yang, Zhao Guangdi, Zang Ximin, Jiang Haoyuan, Wang Zhaoyu.
Effect of Boron on the Microstructure and Strength-Toughness of Fe-Cr-B-C Alloy after Heat Treatment
[J]. Special Steel, 2024, 45(5): 25-33.
|
[12] |
Qu Xiaobo, Wang Miao, Cao Lei, Wang Luyi, Rao Zicai, Ji Wenjie, Wu Yanxin, Wu Xiaoyan, Wang Tianxiang, Jiang Haitao.
Effect of Microstructure Evolution on Mechanical Properties of 87Mnsi Steel Wire Rod for Bridge Cable
[J]. Special Steel, 2024, 45(3): 114-118.
|
[13] |
Chen Yufeng, Zhang Junfen, Xue Qihe, Bai Jun, Yang Shufeng, Li Jingshe.
Effect of Nitrogen Content and Final Rolling Temperature on
Low- temperature Impact Toughness of Titanium
Microalloyed High- strength Steel CGLC700
[J]. Special Steel, 2024, 45(3): 40-18.
|
[14] |
Zhang Yudi, Liu Jianhua, He Yang, Li Wei, Lin Junyu, Chen Xiujun, Bi Sheng.
Industrial Experimental Study on Removal of Inclusions in Steel by Nitrogen Addition and Release Method
[J]. Special Steel, 2023, 44(6): 53-57.
|
[15] |
Xu Letian, Liu Liangyong, Li Yunlong, Xu Yaowen, Wan Wuxia.
Simulation Trial and Finite Element Simulation Study on Temperature Field of Pipes in Walking Beam Reheating Furnace
[J]. Special Steel, 2023, 44(6): 89-95.
|