Abstract: The influence of BaO(2%~8%)on melting and crystalline temperature of concasting mold powder-3~ 5 MgO,1~2 Al₂O₃,8Na₂O,3~4B₂O₃,2Li₂O,3~4 Cand the crystalline phases of free fluoride mold fluxes have been studied and analyzed. The results showed that with increasing BaO content from 2% to 8%,the melting temperature of mold powder decreased obviously from 1053 ℃ to 1011 ℃ while the crystalline temperature decreased minor from 954 ℃ to 948℃;the crystalline mineral phase of free fluoride mold fluxes was melilite which was solid solution of aluminium- melilite(Ca₂Al₂SiO₇),akermanite(Ca₂MgSi₂O₇)and sodium-melilite(NaCaAlSi₂O₇),and it is available through adjustment of crystalline rate of melilite in fluxes to control the heat transfer between mold and shell of strand.
摘要: 实验研究和分析了BaO(2%~8%)对连铸结晶器保护渣(%:3~5MgO、1~2Al2O3、8Na2O、3~4B2O3、2Li2O、3~4C)熔化和结晶温度的影响以及无氟渣的结晶矿相。结果表明,随BaO含量由2%增加至8%,保护渣的熔化温度由1053℃降至1011℃,结晶温度降低较少,从954℃降至948℃;无氟渣的结晶矿相为黄长石,是铝黄长石(Ca2Al2SiO7)、镁黄长石(Ca2MgSi2O7)和钠黄长石(NaCaAlSi2O7)的固溶体,可通过调整渣膜中黄长石的析晶率,控制结晶器与坯壳间的传热。
Dong Fang, Wang Yici , Wang Baofeng. Influence of BaO on Melting Behavior and Crystalline Phase of Concasting Mold Powder[J]. Special Steel, 2006, 27(6): 7-9.
董方, 王艺慈, 王宝峰. BaO对连铸保护渣熔化行为和结晶矿相的影响[J]. 特殊钢, 2006, 27(6): 7-9.