Analysis on Patented Technology of Non-Oriented Electrical Steel Applied in China

Wang Litao1, Zhang Lixia1, Liu Nianhua1, Wang   Quanli1, Wang Xinhua2   

  1. 1 Shougang Research Institute of Technology, Beijing 100041;
    2 School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083
  • Received:2006-07-13 Online:2007-01-01 Published:2023-01-13

在我国申请的无取向电工钢专利技术的分析

王立涛1, 张莉霞1 ,刘念华1, 王全礼1, 王新华2   

  1. 1首钢技术研究院,北京100041;
    2北京科技大学冶金与生态学院,北京100083
  • 作者简介:王立涛(1977-),男,博士,从事炼钢工艺技术研究与电工钢开发。

Abstract: In 1985~2005, the patents of non-oriented electrical steel applied in China consist of 44 patents applied by abroad producers (main producers were JFE and Shin Nippon Seitetsu) and 48 patents applied by native producers (main producers were Baosteel and Wuhan Steel). The fields of patented technology of electrical steel applied by abroad producers mainly include high efficiency and painting technology, and that applied by native producers mainly include rolling process and painting technology. The typical patented technology of non-oriented electrical steel including high efficiency, thin strip casting, painting, shaping process and semi-process products is presented. The developed trend of non-oriented electrical steel is high efficiency production and special service products.

摘要: 1985年至2005年,在我国申请的无取向电工钢专利中,国外厂家有44件,主要为JFE和新日铁;国 内厂家有48件,主要为宝钢和武钢。国外厂家申请的电工钢专利技术领域主要为高效化和涂层技术;国内厂家主 要为轧制工艺和涂层技术。无取向电工钢的典型专利技术:有高效化,薄带连铸、涂层、加工工艺和半工艺产品;无 取向电工钢发展趋势为产品高效化和特殊用途产品。

关键词: 关键词 , 无取向,电工钢, 专利