Grain Refinement Mechanism of 00Cr19Ni10 Austenite by Hot Equal Channel Angular Pressing

Wang   Chang,Yang   Gang,Wang   Limin,Gao   Yongliang   and   Zhong   Hailin     

  1. Structural Material Research Institue, Central Iron and Steel Institute, Beijing 100081
  • Received:2006-08-21 Online:2007-04-01 Published:2023-03-09

等通道热挤压00Cr19Ni10奥氏体不锈钢的晶粒细化机制

王昌, 杨钢,王立民,高永亮,钟海林   

  1. 钢铁研究总院结构材料研究所,北京100081
  • 作者简介:王 昌(1977-),男,工程师,2003年俄罗斯国立莫斯科大学毕业,从事金属材料、透射电子显微技术研究。
  • 基金资助:
    国家863 高技术研究发展计划基金资助项目 (2002AA302501)

Abstract: 150~350 nm super finc grain structure of φ8 mm round stainless steel 00Cr19Ni10-0.025C,18.75Cr, 10.96Ni has been obtained by 8 pass equal channel angular pressing(ECAP)with extrusion speed 9 mm/s at 700 ℃.The  structure evolution of steel in ECAP was analyzed by optical microscope,scanning and transmission electron microscope and X-ray diffraction method. The grain refinement mechanism - dislocation,twins and dynamic recrystallization is proposed and the research discovers that the twins is main grain refining mechanism in 1~4 pass and the dynamic recrystallization is main refining mechanism in 5~8 pass.

摘要: φ8 mm 00Cr19Ni10不锈钢(%:0.025C、18.75Cr、10.96Ni)经700℃、挤压速度9mm/s、8道次等通道 挤压后获得150~350nm 超细晶组织。通过光学显微镜,扫描和透射电镜,X-射线衍射,分析了在等通道挤压变形 过程钢的微观组织演变,提出晶粒细化的位错、孪晶和动态再结晶机制,研究发现在1~4道次以孪晶细化机制为 主,5~8道次以动态再结晶细化机制为主。

关键词: 等通道热挤压法, 奥氏体不锈钢, 晶粒细化机理