ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2007, Vol. 28 ›› Issue (2): 24-25.

Previous Articles     Next Articles

Effect of Aging Temperature on Structure and Properties of 14Co-11Ni- 2Cr-3Mo Secondary Hardening Ultra-high Strength Steel

Li Ani1, Wang Chunxu1, Liu Xianmin1, Zhang Jinghai2, Wang Rui3,Li Jianxin3   

  1. 1 Structural Materials Institute, Central Iron and Steel Research Institute, Beijing 100081;
    2 Technical Center Special Steel Branch, Baosteel, Shanghai 201900;
    3 Technical Center,Dongbei Special Steel Co Ltd, Fushun 113001
  • Received:2006-09-18 Online:2007-04-01 Published:2023-03-09

时效温度对14Co-11Ni-2Cr-3Mo超高强度钢组织与性能的影响

李 阿 妮1, 王 春 旭1,刘宪民1,张 景 海2, 王 瑞3,李 建 新3   

  1. 1钢铁研究总院结构材料研究所,北京100081;
    2宝钢特殊钢分公司技术中心,上海201900;
    3东北特殊钢集团公司技术中心,抚顺113001
  • 作者简介:李阿妮(1978-),女,硕士研究生,2002年北京理工大学材料科学与工程专业毕业,二次硬化型超高强度钢性能研究。

Abstract: Structure and mechanical properties of Co-Ni-Cr-Mo secondary hardening ultra-high strength steel 0. 16C, 11.0Ni,2.0Cr,3.0Mo,14.0Co melted by a 25 kg induction furnace and aged at 460~580 ℃ have been studied. Test results showed that with 860 ℃ quenching + cold treatment at -73 ℃+ aging at 480 ℃,there was large amount dispersed acicular M(Co,Mo)2C precipitates in structure of steel, yield strength Rp0.2 of steel was up to maximum value 1685 MPa, impact energy Akv was 20 J; with overaged condition at 550 ℃,as amount of reverse transformation austenite at lath boundary obviously increased,Akv increased to 32 J and Rp0.2 decreased to 1320 MPa.

摘要: 研究了25 kg感应炉熔炼的Co-Ni-Cr-Mo二次硬化超高强度钢(%:0.16C、11.0Ni、2.0Cr、3.0Mo、14.0Co)经460-580℃时效后的组织和力学性能。试验结果表明,该钢经860℃淬火+(-73℃)冷处理+480℃时效后,组织中存在大量弥散分布的针状M(Co,Mo)2C碳化物,钢的屈服强度Rp0.2达到最大值1 685 MPa,冲击功Akv为20 J;在550℃过时效状态下,板条边界逆转变奥氏体量明显增加,Akv增至32 J,同时Rp0.2下降至1 320 MPa。