Special Steel ›› 2007, Vol. 28 ›› Issue (2): 4-6.

Previous Articles     Next Articles

Study on Mechanism of Elasticity Attenuation of Steel 44Si2CrV Spring

Liu Defu ,Xu Dexiang   

  1. Dongbei Special Steel Group Co Ltd,Dalian 116031
  • Received:2006-10-08 Online:2007-04-01 Published:2023-03-07

44Si2CrV 钢弹簧弹性减退机理的研究

刘德富,徐德祥   

  1. 东北特殊钢集团有限责任公司,大连116031
  • 作者简介:刘德富(1947-),男,博士,教授级高工,从事特殊钢新材料的研究开发。

Abstract: The factors to effect change of free height of steel 44Si2CrV spring during long time loading for 72 h under stress to be lower than yield strength of steel has been studied. The results show that the reduction of free height of steel 44Si2CrV spring under compressive stress 900 MPa consists of two parts: plastic deformation of surface decarburized zone to hinder elastically deformed internal material recovering, making up 84% of total reduction of free height and creep of steel at ambient temperature making up 16% of total reduction of free height.

摘要: 研究了影响44Si2CrV钢弹簧在低于屈服强度的应力下长时间加载引起自由高度变化的因素。结果表明,44Si2CrV钢弹簧在900 MPa 的应力下压缩72 h,自由高度的缩短由两部分组成:表面脱碳层的塑性变形,造成对内部材料的牵制而使部分弹性变形不能恢复,由此所造成的弹簧自由高度缩短占总变形量的84%;钢的室温蠕变,占自由高度缩短的16%。