Structure and Composition in Boronizing Layer of Steel Cr12MoV

Miao Quansheng, Hao Shaoxiang   

  1. Department  of  Mechanical  and  Electronic  Engineering,Henan  Engineering  Institute,Zhengzhou  450053
  • Received:2008-01-16 Online:2008-08-01 Published:2022-12-23

Cr12MOV钢渗硼层的组织和成分

苗全生, 郝少祥   

  1. 河南工程学院机电系,郑州450053
  • 作者简介:苗全生(1953-),男,副教授,1976年北京工业学院毕业,机械设备检测与维修方面的研究和教学。

Abstract: The  change  of structure  and  element  content in boronizing layer of steel  1.72C- 11.81Cr-0.40Mo has been analyzed  and  studied  by  using  optical  microscope,scanning  electron  microscopy  and  X-ray  analyzer. Results  showed  that the  boronizing  layer  consisted  of  white-bright  boronizing  zone(phase  FeB-phase  Fe₂B)and  black  alternating  with  white transition  zone;  there  was  a  lot  of  irregular  island  B  bearing  carbides;and  there  were  the  elements  such  as  B,C,Al,Si, Mo,Cr,Fe  in  boronizing  layer,the  B,Cr  and  Fe  content  at  front  of boride  in  boronizing  layer  was  11.48%,36.49%  and 32.23%  respectively  while  the   B,Cr   and   Fe   content   in  transition   zone  was8.07%,7.04%   and77.21%  respectively, but the Mo content was almost no change.The Cr and Mo existed in boronizing layer by carbides form,and Al and Si existed  at defect or high carbon area in boronizing layer.

摘要: 用光学显微镜、扫描电子显微镜和X-射线仪分析和研究了1.72C-11.81Cr-0.40Mo钢渗硼层组织和元素含量的变化。结果表明,渗硼层由白亮的硼化区(FeB相-Fe2B相)和黑白相间的过渡区组成;硼化区前端存在大量形状不规则的岛屿状含硼碳化物。渗硼层中存在B、C、Al、Si、Mo、Cr、Fe等元素,硼化物前端的B、Cr、Fe含量分别为11.48%、36.49%和32.23%,过渡区的B、Cr、Fe含量分别为8.07%、7.04%和77.21%,而Mo含量几乎没有变化。渗硼层中Cr、Mo以碳化物形式存在,Al、Si存在于缺陷处或高碳区中。