Progress in Equipment Technology of 100~300 t Large Converter

Guo Hong1 , Chen Linquan1 , Tian Weida1 , Zhao Lisong2   

  1. 1. Hua Tian Engineering Research Incororation Limited,Maanshan 243005;
    2. Rongsheng Project Department, Shagang Group,Zhangjiagang 215600;
  • Received:2008-03-16 Online:2008-10-01 Published:2023-01-05

100~300 t大型转炉设备技术的进展

郭 红1,陈林权1,田伟达1,赵立松2   

  1. 1. 中冶华天工程技术有限公司炼钢室,马鞍山 243005;
    2. 江苏沙钢集团荣盛项目部,张家港 215600;
  • 作者简介:郭红(1981-),女,硕士,助理工程师,2006年重庆大学毕业,炼钢工艺设计。

Abstract: At present the main advances in equipment technology of 100~300 t large converters are application of creep-resistant material 16Mo3 at elevated temperature 550 ℃ for converter shell; application of steel P285NH and P420NH for converter trunnion and ring; natural air cirular cooling trunnion; unique water cooling upper cone technology; and maintenance-free link rod suspension system.

Key words: Large Converter, Equipment Technology, Progress

摘要: 目前100~300 t大型转炉设备技术的进展主要有:550℃高温抗蠕变材料16Mo3在转炉炉壳上的应用;P285NH、P420NH钢在托圈和耳轴的应用,自然的空气循环冷却托圈;独特的水冷炉帽技术;免维护的连杆式下悬挂系统。