A Study on Water Simulation for Optimizing Tundish Structure  and Inclusion Removal in Concasting

Gao Jinguo, Li Jingshe, Tang Haiyan , Yang Shufeng   

  1. School of Metallurgical and Ecological Engineering, University Science and Technology, Beijing 100083
  • Received:2008-07-22 Online:2009-02-01 Published:2022-11-29

连铸中间包结构优化及夹杂物去除的水模拟研究

高锦国, 李京社, 唐海燕, 杨树峰   

  1. 北京科技大学冶金与生态工程学院,北京100083
  • 作者简介:高锦国(1980-),男,助理工程师,硕士生,北京科技大学毕业,主要从事钢的洁净度研究。

Abstract: According to prototype 25 t tundish, the liquid flow field and the removal of inclusions in an approximate rf-shape tundish with three kind卜 of weirs in 4-strarid easting have been analyzed by using experimental similarity ratio λ= 1 : 2. 3 uatrr model. Results showed that by using original weir, there was a great differrm-r in (low characteristics between I wo outlets at the same hide of tundish, ami compared t。inside outlet the outside outlet had longer minimum residence lime and peak time and large dead zone volume led to liquid temperature variation and delaying inclusion floatation; by using U- type weir, the peak time could be prolonged, but with short minimum residence time and large dead zone volume; and bv lining -shape weir it was available to efficiently change the liquid flow distribution in tundish and improve inclusion removal. The conimercial test for steel 30CrMo indicated that with using Y-weir the large inclusion amount in steel decrrasrtl by 16. 9% as co in pared with using original wrir.

摘要: 以25t中间包为原型,通过实验相似比λ=1:2.3的水模型,分析了4流近似T型中间包3种挡墙形式包内流场及夹杂物去除。结果表明,原挡墙控流下的中间包同一侧两流之间的流体流动特性差异很大,与内侧相比,外侧流的最短停留时间和峰值时间长、死区体积大,造成中间包内钢液温度不均匀,夹杂物不能有效地上浮去除;U-型挡墙能延长峰值时间,但是最短停留时间短,死区比例较大;采用Y-型挡墙可以有效地改变中间包内流场分布,促进夹杂物上浮。30CrMo钢工业试验表明,采用Y-型挡墙钢中大型夹杂物较原用挡墙降低16.9%。