ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2009, Vol. 30 ›› Issue (1): 29-31.

Previous Articles     Next Articles

A Study on Model of Steelmaking Process for Stainless Steel by AOD

Li Shiqi1 , Jiang Guoli1,2, Lu Junping1, Lin Gang3   

  1. 1 School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083 ;
    2 Haicheng Dongsi Section Steel Co Ltd, Haicheng 114200 ;
    3 IkeLuoGap (Beijing) International Investment Advisory Co Ltd, Beijing 100070
  • Received:2008-07-09 Online:2009-02-01 Published:2022-11-29

AOD冶炼不锈钢工艺模型的研究

李士琦1, 江国利1,2, 路俊萍1, 林纲3   

  1. 1北京科技大学冶金与生态工程学院,北京100083;
    2海城市东四型钢有限公司,海城114200;
    3艾克罗盖普(北京)国际投资咨询有限公司,北京100070
  • 作者简介:李士琦(1942-),男,教授.《特殊钢》编委,钢铁冶金研究疽

Abstract: Based on practical production data of steelmaking process for 304 stainless steel by a 45 t AOD-L unit, according to system modeling, conservation of mass and energy, and thermodynamic principle, a processing model (AOD M&H) for austenite stainless steel steelmaking by AOD process has been established including four levels: operation, chemical reaction, metallurgy and energy computation with 469 variables. With 139 input variables including amount, ingredient and temperature of each material, the 39 output variables such as chemical composition and temperature of liquid steel etc. can be calculated by the model. Application results showed that the relative error of carbon content and temperature of liquid steel in each phase of steelmaking process between calculated and measured value was ≤11. 1 %.

Key words: Stainless Steelmaking, AOD, Process Model

摘要: 以45t AOD-L冶炼304不锈钢的实际生产数据为依据,根据系统模化、质量、能量守恒及热力学原理,建立了AOD冶炼奥氏体不锈钢的工艺模型(AOD M&H),包含操作、化学反应、冶金计量和热化学计量4个层次,共涉及469个变量。使用该模型进行模拟,由139项输入变量,包括各物料的用量、成分和温度,可方便地求出39项输出变量,如钢液成分、温度等。应用结果表明,冶炼过程中各阶段的钢液碳含量与温度的预报值和实测值的相对误差≤11.1%。

关键词: 不锈钢冶炼, AOD, 工艺模型