A Study on Water Modeling of Fluid Flow in a Tundish for Horizontal Continuous Casting
Yang Shufeng1, Li Jingshe1, Tang Haiyan1, Shi Shaoqing1,2
1 School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083;
2 Hengyang Steel Tube Co Ltd, Hengyang 421001
Yang Shufeng , Li Jingshe, Tang Haiyan, Shi Shaoqing. A Study on Water Modeling of Fluid Flow in a Tundish for Horizontal Continuous Casting[J]. Special Steel, 2009, 30(4): 22-23.