Practice of Process for Improving Yield of Seamless Pipe Hot-Rolled by 114CPE Mill

Zhuo Zhao1,Hang Naiqing1,Cheng Xianglong1,Duan Jiatian2,Kang Zhiyong2   

  1. 1Collegeof Materials and Metallurgy,Wuhan Universityof Science and Technology,Wuhan 430081:
    2Hanyang Steel Rolling Plant,Wuhan Iron and Steel,Wuhan 430035
  • Received:2009-05-18 Online:2009-12-01 Published:2022-11-15

提高114CPE机组热轧无缝钢管成材率的工艺实践

卓 钊1,杭乃勤1,程向龙1,段家田2,康志勇2   

  1. 1武汉科技大学材料与冶金学院,武汉430081;2武钢汉阳轧钢厂,武汉430035
  • 通讯作者: 杭乃勤
  • 作者简介:卓 钊(1981-),男,硕士研究生,金属加工过程组织和性能控制。

Abstract: In light of the problem of low yield of pipe for petroleum produced by Φ114mm cross roll piercing elongation(CPE)mill,an analysis on production process flow sheet has been carried out.  It is obtained that hot-sawing on pipe in middle procedure and hot-cutting ends are two factors led to low yield. With adopting the improved alignment method as pipe moved to cooling bed and the  pointing  process,the  comprehensive yield of Φ73.0  mm×5.5 mm and P88.9 mm× 6.5 mm pipes for petroleum increases to84.5%~85.0% from original 78%

Key words: CPE Mill,Bush Bench,Mandrel,Pointing Process,Yield

摘要: 针对Φ114mm CPE(斜轧穿孔延伸)机组生产石油用管成材率低的问题,对生产工艺流程进行了分析。得出中间热锯切和热切头尾是导致成材率低的两个重要原因。通过采用改进的钢管下冷床对齐方法以及缩口工艺,使Φ73.0 mm×5.5 mm和Φ88.9 mm×6.5 mm的石油用管综合成材率由78%提高至84.5%~85.0%。

关键词: CPE机组, 顶管机 , 芯棒, 缩口工艺, 成材率