Pilot Production of 0300 mm Round Casting Bloom of X65 Pipeline Steel at Baogang

Ma Xiaoguang1, Wang Tianyao2 ,  Zhang Xiuping2   

  1. 1 Planning and Developing Dept, Baotou Iron & Steel (Group) Co Ltd, Baotou 014010;
    2 Steelmaking Plant, Steel Union Co Ltd, Baotou Iron & Steel (Group) Co Ltd, Baotou 014010
  • Received:2009-10-09 Online:2010-04-01 Published:2022-11-16

包钢X65管线钢Φ300 mm圆铸坯的试制

麻晓光1, 王天瑶2, 张秀平2   

  1. 1包钢(集团)公司规划发展部,包头014010;
    2包钢钢联股份有限公司炼钢厂,包头014010
  • 作者简介:麻晓光(1968-),男,硕士,高级工程师,1991年内蒙古科技大学毕业,精炼和连铸工艺研究。

Abstract: The X65 pipeline steel 13MnNbTi (% : 0. 10 ~Q 16C, 1.20 ~ 1.40Mn, 0. 03 ~0. 05Nb, 0.01 ~0. 02Ti, 0.025 ~0. 05Al) is pilot-produced by 120 t top and bottom combined blown converter-100 t LF (VD) -5 strands Φ300 mm round bloom casting flow sheet at steelmaking plant, Baotou Steel Union Co Ltd. Production practice shows that it is available by desulphurization of hot metal ([S] ≤0. 005% ) , using slag stopper during converter tapping, basicity of refining slag ≥3. 0, VD treatment ≥13 min, to get [S]≤0. 005% , [P] ≤0. 015% and [ H] ≤1.5 x 10-6. With shielding casting in whole process and mold electromagnetic stirring, the oxygen content in steel is (13 ~21) x I0-6, average oxygen content is 16. 44 x 10-6, the surface quality of bloom is fine and the rating of macrostructure is 0 ~ 1.

Key words: X65 Pipeline Steel, 6300 mm Round Cast Bloom, Process Practice

摘要: 包钢钢联股份有限公司炼钢厂采用120 t顶底复吹转炉-100 t LF(VD)-5流Φ300 mm铸坯连铸工艺流程试生产X65管线钢13MnNbTi(%:0.10~0.16C、1.20~1.40Mn、0.03~0.05Nb、0.01~0.02Ti、0.025~0.05Al)。生产实践表明,通过铁水脱硫([S]≤0.005%),转炉挡渣出钢,精炼渣碱度≥3.0,VD处理≥13 min,可以使[S]≤0.005%、[P]≤0.015%、[H]≤1.5×10-6。通过全程保护浇铸和结晶器电磁搅拌工艺,钢中氧含量(13~21)×10-6,平均氧含量16.44×10-6,铸坯表面质量良好,低倍组织0~1级。