A Study on Melting Temperature of Pentatomic Refining Slag Series
Li Shiqi1 , Li Jin1, 2, Liu Jinxia1 , Zhang Yanyan1 , Pang Yonggang3 , Wang Huizhong1
1 School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083 ;
2 Beijing Municipal Research Institute of Environmental Protection, Beijing 100037 ;
3 Beijing Keda Fangxin High and New Technology Co Ltd, Beijing 100083
Li Shiqi , Li Jin, Liu Jinxia , Zhang Yanyan , Pang Yonggang, Wang Huizhong. A Study on Melting Temperature of Pentatomic Refining Slag Series[J]. Special Steel, 2010, 31(3): 1-2.
1张鉴.CaO-SiO2渣系作用浓度的计算模型.北京钢铁学院学 报,1988,10(4) :412
2Turkdogan E T. Slag and Fluxes for FeiTous Ladle Metallurgy, Iron and Steelmaking, 1985,12(2) ;64
3Hideaki Suito, Hajime Inoue, Ryo Inoue. Aluminium-Oxygen Equilibrium Between CaO-Al2O3 Meltss and Liquid Iron, Iron & Steelmaking, 1991,31(12):1389
4东方人华,周 皓.统计基础和SPSS 11.0 入门与提高.北京:清 华大学出版社,2004
5试验设计法讲义.北京:北京大学出版社,1966