Previous Articles     Next Articles

Development Trend of Overseas Drill Pipe Products

Zhao   Peng1,2,  Li   Jun1,2   

  1. 1 School  of Materials and  Metallurgy, Northeastern  University, Shenyang  110004;
    2 Baoshan iron and Steel  Co  Ltd,Shanghai  201900
  • Received:2010-01-20 Online:2010-08-01 Published:2022-11-20

国外钻杆产品发展动向

赵 鹏1,2 李俊1,2   

  1. 1东北大学材料与冶金学院,沈阳110004;2宝山钢铁股份有限公司,上海201900
  • 作者简介:赵 鹏(1974-),男,博士生,高级工程师,油井管新产品开发

Abstract:  Drill   Pipe   is   main   component   part   of   oil   drill-stem, its   service   environment   is   extremely   severe   and   stress conditions   are   very   complicated.   The   development   trend   of   overseas   drill   pipe   products   is   presented   from   both   development of   drill   pipe   grades   and   connector   including   ultra-high   strength   drill   pipe, sour   service   drill   pipe, titanium   alloy   drill   pipe, intelligent   drill   pipe, ultra-high   torque   tool   joint   and   fast   make-up   ultra-high   torque   tool   joint.

摘要: 钻杆是石油钻柱的主要组成部分,服役环境异常苛刻,受力状态十分复杂。从钻杆品种的发展、钻杆扣型的发展两方面介绍国外钻杆产品的发展动向,内容包括超高强度钻杆、抗硫钻杆、钛合金钻杆、智能钻杆、超高抗扭接头以及快速上扣超高抗扭接头。