A Test and Study on Water Modelling for Optimization of Bottom Argon Blowing Process of a 90 t Ladle Furnace
Ding Ning1,2 , Bao Yanping1 , Sun Qisong2 , Wang Lifeng2
1. School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083 ;
2. Shougang Research Institute of Technology, Beijing 100043 ;
Ding Ning , Bao Yanping , Sun Qisong , Wang Lifeng. A Test and Study on Water Modelling for Optimization of Bottom Argon Blowing Process of a 90 t Ladle Furnace[J]. Special Steel, 2010, 31(5): 8-10.