Special Steel ›› 2011, Vol. 32 ›› Issue (2): 11-14.

Previous Articles     Next Articles

Development of Prediction Model for Temperature of Liquid Steel in 120 t LF at Shaosteel

Xiao Chaoping1 , Bao Yanping2, Yuan Pengfei2, Liu Zhiming1,3, Cheng Xiaowen3, Qiu Wensheng3   

  1. 1 School of Metallurgical and Ecological Engineering,
    2 Research Institute of Metallurgical Engineering, University of Science and Technology, Beijing 100083 ;
    3 Shaoguan Iron and Steel Group Co Ltd, Shaoguan 512123
  • Received:2010-11-19 Online:2011-04-01 Published:2022-11-08

韶钢120 t LF钢水温度预报模型的开发

肖超平1,包燕平2, 元鹏飞2, 刘志明1,2, 程晓文3, 丘文生3   

  1. 北京科技大学1冶金与生态工程学院,
    2冶金工程研究院,北京100083;
    3韶关钢铁集团有限公司,韶关512123
  • 作者简介:肖超平(1987-),男,硕士研究生,钢铁冶金研究。

Abstract: According to the studied system of liquid steel, refining slag and alloy in 120 t LF refining process, based on energy-balance principle model the prediction model for temperature of refining liquid steel has been established. According to steel grade, liquid weight and temperature, aim tapping temperature and treated time, adding amount of refining slag material and alloys as well as various heat loss to get required input electric energy, the reasonable electric supply curves during refining are determined. And the temperature of liquid is predicted according to parameters of electric supply and process at worksite. Examination results on 20 heats steel 50RH1 (% : 0. 48C ~ 0. 50C, 0. 22 ~ 0. 30Si, 0. 60 - 0. 70Mn) show that the error of temperature of liquid between model predicted value and measured value are ±5℃.

Key words: LF Refining, Temperature of Liquid, Prediction Model

摘要: 以钢厂120 t LF精炼过程钢水、炉渣和合金为研究体系,以能量平衡机理模型为基础,建立精炼钢水温度预报模型。根据钢种、钢水质量和温度、目标出钢温度及处理时间、渣料和合金加入量及各种热损失所需投入的电能,确定精炼过程合理的供电曲线。并根据现场供电和工艺参数,预报钢水温度。20炉50RH1钢(%:0.48~0.50C、0.22~0.30Si、0.60~0.70Mn)测试结果表明,模型预报与实测钢水温度误差为±5℃。

关键词: LF精炼, 钢水温度, 预报模型