ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2011, Vol. 32 ›› Issue (3): 65-67.

Previous Articles     Next Articles

A Study on Crevice Corrosion Performance of 445M Ferrite Stainless Steel

Gu Yue1 , Zhan Zhaolin1 , Rong Fan   

  1. 1 Kunming University of Science and Technology, Kunming 650093 ;
    2 Central Iron and Steel Research Institute, Beijing 100081
  • Received:2010-12-15 Online:2011-06-01 Published:2022-10-18

445M铁素体不锈钢缝隙腐蚀性能的研究

顾玥1,詹肇麟1,荣凡2   

  1. 1昆明理工大学,昆明650093 ;
    2钢铁研究总院,北京100081
  • 通讯作者: 詹肇麟,教授,昆明理工大学莲华校区,昆明650093 荣凡,教授,北京钢铁研究总院,北京100081
  • 作者简介:顾 明(1984-),女,研究生,445铁素体不锈钢应用性能研究。
  • 基金资助:
    国家科技部支撑计划项目资助(2007BAES1B01).

Abstract: The crevice corrosion performance of 445M ferrite stainless steel ( % : 0. 004 ~0. 005C, 22. 4 - 22. 29Cr, 1. 10 ~ 1. 65Mo, 0. 015 ~0. 016P, 0. 003 ~0. 004S, 0. 012 -0. 016N, 0. 22 - 0. 38Ti) and 316L austenite stainless steel ( % : 0. 022C, 16. 80Cr, 10. 19Ni, 2. 02Mo, 0. 025P, 0. 001S, 0. 046N) in sodium chloride solution with chlorion concentration (250 - 5 000) x 10-6 at 40 ~ 60 ℃ has been studied. Results show that the crevice corrosion resistance of 445M steel is better than that of 316L steel ; and with increasing the Mo content in 445M steel from 1. 10% to 1. 65% , the crevice corrosion resistance of steel obviously increases, it indicated that the pitting corrosion resistance equivalent- Cr +3. 3Mo is an important index to measure the pitting and crevice corrosion resistance of stainless steels.

Key words: 445M Ferrite Stainless Steel, Crevice Corrosion, Pitting Corrosion Resistance Equivalent

摘要: 研究了445M铁素体不锈钢(%:0.004~0.005C、22.24~22.29Cr、1.10~1.65Mo、0.015~0.016P、0.003~0.004S、0.012~0.016N、0.22~0.38Ti)和316L奥氏体不锈钢(%:0.022C、16.80Cr、10.19Ni、2.02Mo、0.025P、0.001S、0.046N)在40~60℃氯离子浓度(250~5 000)×10-6的氯化钠溶液的缝隙腐蚀性能。结果表明,445M铁素体不锈钢的耐缝隙腐蚀性能优于316L奥氏体不锈钢;当445M钢中的Mo含量由1.10%提高至1.65%时,钢的耐缝隙腐蚀性能明显提高,表明点蚀当量Cr+3.3Mo是衡量不锈钢耐点蚀和耐缝隙腐蚀的重要指标。