Special Steel ›› 2011, Vol. 32 ›› Issue (4): 14-17.

Previous Articles     Next Articles

Numerical Simulation and Metallurgical Effect for Structure Optimization of 6-Strand Tundish for 12-Strand Casting Billets

Han Chuanji1, An Hanghang1, Ji Wei1, Li Fushuai1, Tao Jinming1, Wang Jianfeng2 , Jia Jianping2   

  1. 1 Beijing Metallurgical Technology Research Institute, CCTEC, Beijing 100028 ;
    2 Steelmaking Works, Xuanhua Steel Co, HBIS, Zhangjiakou 075100
  • Received:2011-03-18 Online:2011-08-01 Published:2022-10-31

12流小方坯6流中间包结构优化的数值模拟和冶金效果

韩传基1, 安航航1, 季维1, 李富帅1, 陶金明1, 王剑峰2,贾建平2   

  1. 1中冶连铸北京冶金技术研究院,北京100028;
    2河北钢铁集团宣钢公司炼钢厂,张家口 075100
  • 作者简介:韩传基(1966-),男,博士,研究员,2006年北京科技大学毕 业,钢的质量控制和连铸新工艺研究:

Abstract: The three-dimensional flow field, concentration field and temperature field of a 35 t 6-strand tundish for 12-strand 150 mm x 150 mm continuous machine at Xuanhua Steel have been studied by using numerical simulation and the optimum flow control device slag dam with hole diameter 120 mm, horizontal deviation angle 5° and vertical angle of elevation 5° is obtained. Application Results show that the flow field in structure-optimized tundish improved obviously, the flow behavior of each strand of tundish becomes consistent, the impacting of liquid on 6-th strand stopper is alleviated, the temperature difference between each strand decreases to 4 K from original 10 K and the continuous casting time increases to 26 h from original 20 h.

Key words:  , 12-Strand Casting Billet, Tundish for 6-Strand, Structure Optimization, Numerical Simulation

摘要: 利用数值模拟对宣钢12流150mm×150mm连铸机的35 t 6流中间包的三维流场、浓度场和温度场进行研究,得出了最佳控流装置挡渣墙孔径120 mm,水平偏角5°,竖直仰角5°。应用结果显示,优化结构中间包的流场明显改善,各流的流动特性趋于一致,钢液对第6流塞棒的冲击减轻,各流最大温差由原先的10 K降低至4K。且连浇时间由原先的20h延长到26h。

关键词: 12流小方坯, 6流中间包, 结构优化, 数值模拟