Research and Production of Φ508 mm x 50 mm WB36 Steel Tube with Pilger Rolling Process

Wang Yong , Ran Xu , Zhang Min   

  1. Hunan Hengyang Steel Tube (Group) Co Ltd, Hengyang 421001
  • Received:2011-05-10 Online:2011-10-01 Published:2022-11-04

周期轧管工艺生产Φ508 mm x 50 mm WB36钢管的研制

王勇,冉旭,张敏   

  1. 湖南衡阳钢管(集团)有限公司,衡阳 421001
  • 作者简介:王勇(1982-),男,硕士,工程师,2007年武汉科技大学毕业,轧钢新工艺、新产品研究。

Abstract: Metallurgical flow sheet for production of WB36 steel tube (%: 0.16C. 0.46 ~0.47Si, 1.02 ~ 1.05 Mn , 0.008 〜0.010P, 0. 001S, 0.29 ~0.30Mo, 1.17〜1.20N、0.58Cu, 0.02M), 0.05Al) is 45 t EAF-LF-VD-Φ600 mm casting bloom-piercing, Φ600 m×70 mm-Φ720 Pilger mill rolling. With controlling heating atmosphere in circular rotating furnace, temperature at soaking zone 〜1 250  , piercing temperature 1 100 °C , then blank lube tolling with three-dimensional stress by Pilger Mill, the structure of quenched-tempered WB36 steel tube is ferrite + bainite, its mechanical properties at ambient and elevated temperature, and weldability all meet the requirement of EN10216-2 standard.

Key words: WB36 Steel Tube, Large Caliber, Pilger Rolling, Research and Production

摘要: WB36钢管(%:0.16C、0.46~0.47Si、1.02~1.05Mn、0.008~0 010P、0.00IS、0.29~0.30Mo、1.17~1.20Ni、0.58Cu、0.02Nb、0.05 Al)冶金流程为45 t EAF-LF-VD-Φ600 mm铸坯-穿孔,Φ600 m×70 mm-Φ720周期轧管机组轧制.通过控制环形炉加热气氛,均热段温度~1 250℃,穿孔温度1 100℃,随后毛管在周期轧管机中以三向压应力状态进行轧制,WB36钢管淬-回火后的组织为铁素体+贝氏体,室温和高温力学性能以及焊接性能均符合EN10216-2标准要求

关键词: WB36钢管, 大口径, 周期轧管, 试制