Practice of Production Process for 300 mm x 300 mm EA4T Axle Steel Bloom

Zhang Chunhong, Yang Jieming, Tang Xueping   

  1. Technology Center, Shougang-Guiyang Special Steel Co Ltd, Guiyang 550005
  • Received:2011-09-05 Online:2012-02-01 Published:2022-09-20

300 mm x300 mm EA4T车轴钢坯生产工艺实践

张春红, 杨接明, 唐雪萍   

  1. 首钢贵阳特殊钢有限责任公司技术中心,贵阳550005
  • 作者简介:张春红(1971-),女,主任工程师,硕士,1993年北京科技大学毕业,锻造工艺研究及产品标准管理。
  • 基金资助:
    国家科技支撑计划,编号2007BAE11B01 ;黔科合重大专项,编号20066031

Abstract: The EA4T axle steel (/% : 0. 22 ~ 0. 29C, 0. 15 ~ 0. 40Si, 0. 50 ~ 0. 80Mn, ≤0. 020P, ≤0. 015S, 0. 90 ~ 1. 20Cr, 0. 15 ~0. 30Mo, ≤0. 06V) is produced by 30 t EBT arc furnace-40 t LF/VD-5 t ingot process and forged by 8MN oil-hydraulic press to 300 mm x300 mm bloom with forging ratio ≥9. Results show that of the EA4T steel, [0] is (12 ~ 15) x 10-6, [ H] is (1. 2 ~ 1. 6) x 10-6, with quenching at 900 - 920 °C and tempering at 600 ~650 °C, tensile strength Rm721 ~745 N/mm2, yield strength ReH 463 ~470 N/mm2, elongation A5 19. 0% ~ 19. 5%, longitudinal impact energy 53 ~73 J, transverse impact energy 36 ~41 J, structure is bainite-tempered martensite, and 107 cycle fatigue limit is 350 N/mm2.

摘要: EA4T车轴钢(/%:0.22~0.29C、0.15~0.40Si、0.50~0.80Mn、≤0.020P、≤0.015S、0.90~1.20Cr、0.15~0.30Mo、≤0.06V)采用30 t EBT电弧炉40 t LF/VD-5 t铸锭工艺生产,并经8 MN油压机锻成300 mm x300mm钢坯,锻造比≥9。结果表明,EA4T钢[O]为(12-15)×10-6,[H]为(1.2~1.6)×10-6,经900~920℃淬火,600~650℃回火后,抗拉强度Rm721~745 N/mm2,屈服强度ReH463~470 N/mm2,伸长率A5 19.0%~19.5%,纵向冲击功53~73 J,横向冲击功36~41 J,组织为贝氏体一回火马氏体,10~7循环疲劳极限为350 N/mm~2。