Hydraulic Simulation of Optimization of Flow Control Devices for a Tundish of Eight-Strand Continuous Casting

Wang Hongbin, Tang Haiyan, Li Jingshe , Bai Liguo   

  1. School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083
  • Received:2012-01-30 Online:2012-06-01 Published:2022-10-13

八流连铸中间包控流装置优化的水力学模拟

王宏斌,唐海燕 ,李京社, 白李国   

  1. 北京科技大学冶金与生态工程学院,北京100083
  • 作者简介:王宏斌(1968-),男,博士研究生,钢的质量控制硏究。
  • 基金资助:
    国家自然科学基金(No. 51074021 )、教育部博士点 基金(No. 20100006120008 )和博士后基金项目 (20100480204)资助。

Abstract: The flow field of in a 40 t tundish with different flow control devices for eight-strand continuous casting has been simulated by test of water model with 1-3.5 geometric similarity scale. Results show that the average stagnation time of original tundish is short and the difference of residence time between four outlets at one side of tundish is large ; as compared original tundish the dead area volume fraction of tundish with optimum weir and double diversion holes and with optimum C12W1 rectangle weir respectively decreases by 19. 15% and 31. 49% , and the difference value of stagnation time between four outlets at one side also decreases ; the installed turbulence modifier can increase stagnation time and peak time of molten steel, but not effectively reduce the dead area volume fraction.

摘要: 通过几何相似比1:3.5的水模型实验对40 t八流中间包不同控流装置下的流场进行了模拟研究。结果表明,原中间包平均滞止时间短,一侧4个水口的停留时间相差较大;优化的双导流孔挡墙可使中间包死区体积分数比原型减少19.15%,优化的C12W1矩形挡墙可使中间包死区体积分数比原型减少31.49%;中间包一侧4个水口的滞止时间差值减少;设置湍流抑制器虽然增加钢液的滞止时间和峰值时间,但不能有效地降低死区体积分数。

关键词: 八流中间包, 水模型, 挡墙, 湍流控制器, 优化设计