1 JFE. Cr-Containing Steel Pipe Having Excellent High Pressure Carbon Dioxide Corrosion Resistance : JP. JP2010111930. [DB/OL]. 2008- 11-07[2010-05-201. http:〃wwwl9. ipdL inpit. go. jp/PAl/cgi-bin/ PAI DETAIL
2 JFE. Seamless Pipe of Martensitic Stainless Steel for Oil Well Pipe and Process for Producing the Same: JP. JP2010168646. [DB/OL]. 2009-09-02 [2010-08-05]. http:// www 19. ipdl. inpit. go. jp/PAl/ cgi-bin/PAl DETAIL
3 JFE. High-Strength Stainless Steel Pipe Having High Toughness and Excellent Corrosion Resistance for Oil Well :JP. JP2010209402. [DB/ OL]. 2009-03-10 [2010-09-24]. http:// wwwl9. ipdl. inpit. go. jp/
PA1/cgi-bin/PA1 DETAIL
4 JFE. Method for Manufacturing Martensitic Stainless Steel Seamless Steel Tube for Oil Well Pipe:JP. JP2010242163. [ DB/OL]. 2009- 04-06[ 2010-10-28 J. http: //wwwl9. ipdl. inpit. go. jp/PAl/cgi-bin/ PA1 DETAIL
5 JFE. Seamless Pipe of Martensitic Stainless Steel for Oil Well Pipe and Process for Producing the Same: WIPO. W02010026672. [DB/OL] 2008-12-24 [ 2010-03-11 ] : http; // worldwide, espacenei. com/ publicationDetails/biblio? DB = EPODOC&II = 0&ND 二 3&adjacent =true&locale = en^EP&FT = D&date = 20100311 &CC = WO&NR = 2010026672Al&KC = Al
6 JFE. High-Strength Seamless Steel Tube for Use In Oil Wells, Which Has Excellent Resistance to Sulfide Stress Cracking and Production Method for Same: WIPO. W02010150915. [DB/OL]. 2010-06-23 [2010-12-29 ]. http: // worldwide, espacenet. com/publicalionDr- tails/biblio? DB = EPODOC&II = 0&ND = 3&adjacent = true&locale = en _ EP&FT = D&date = 20101229&CC = WO&NR = 2010150915A1&KC = Al
7 JFE. Method for Manufacturing Circumferential Weld Joint of Martensitic Stainless Steel Tube:JP. JP2010029941. [DB/OL]. 2009-08-24 [2010-02-12]. http: // wwwl9. ipdl. inpit. go. jp/PAl/cgi-bin/ PAI DETAIL
8 Sumitomo Metal Industries Ltd. High Strength Stainless Steel Piping Having Outstanding Resistance to Sulphide Stress Cracking and Resistance to High Temperature Carbon DioxideCorrosion: WIPO. W02010050519. [ DB/OL], 2009-10-28 [ 2010-05-06 J. http: // worldwide. espacenet. com/ publicationDetails/biblio? DB = EPODOC&II = 0&ND = 3&adjacent = tme&locale = en_EP&KP = D&date = 20100506&CC = WO&NR =2010050519 Al &KC = Al
9 Sumitomo Metal Industries Ltd. Stainless Steel for Oil Well, Stainless Steel Pipe for Oil Well, and Process for Production of Stainless Steel for Oil Well: WIPO. WO2010134498. [ DB/OL]. 2010-05-17 [ 20i0- 11 -25 ]. http: 〃worldwide, espacenet. com/publicationDetails/bibljo? DB = EPODOC&II = Q&ND = 3&adjacent = true&locale = en_EP&FT = D&date =20101125&CC = WO&NR =2010134498Al &KC = Al
10 Sumitomo Metal Industries Ltd. The Manufacturing Method of a Duplex-Stainless-Steel Pipe I Tube:JP. JP04462454. [ DB/OL]. 2009- 11 -02 [ 2010-05-12 ]. http: // wwwl9. ipdl. inpit. go. jp/PAl/cgi- bin/PAl DETAIL
11 Sumitomo Metal Industries Ltd. The Manufacturing Method of the High Strength Cr-Ni Alloy Seamless Pipe:JP. JP04553073. [ DB/ OL]. 2010-03-29 [ 2010-09-29 ]. http: // www 19. ipdl. inpit. go. jp/ PAI/cgi-bin/PAl DETAIL
12 Sumitomo Metal Industries Ltd. The Manufacturing Method of A High-Alloy Pipe I Tube: JP. JP04462452. [ DB/OL J. 2009-0M9 [2010-05-12 ]. http: // wwwl9. ipdl. inpit. go. jp/PAl/cgi-bin/ PAI DETAIL
13 Vallourec Mannesmann Oil & Gas. Low Alloy Steel With A High Yield Strength and High Sulphide Stress Cracking Resistance: F'R. FR2942808. [DB/OL]. 2009-03-03〔 2010-09-10], http: // worldwide. espacenet. com/publicationDetails/biblio? DB = EPODOC&II -0&ND = 3&adjacent = true&locale = en _ EP&FT = D&dalt= 20100910&CC = FR&NR =2942808Al&KC = Al
14 Vallourec Mannesmann Oil & Gas. Low Alloy Steel With A High Yield Strength and High Sulphide Stress Cracking Kesistance: WIPO. W02010066584. [DB/OL]. 2009-11-25 [ 2010-06-17 ]. http: // worldwide, espacenet. corn/publieationDetails/biblio? DB = EPODOC&II = 0&ND = 3&adjacent = true&locale = en_EP&FT = D&date =20100617&CC = WO&NR = 2010066584Al&KC = Al
15 宝钢.一种耐热套管用钢及其制造方法. CN. 101748330 [DB/ OL]. 2008-12-17 [ 2010-06-23 ]. http: //search, cnipr. com/search, do? method = detailSearch
16 宝钢.一种石油套管及其制造方法.CN. 101845939 [DB/OL]. 2009-03-25 [ 2010-09-29 ]. http: // search, cnipr. com/search, do? method = detailSearch
17 宝钢.抗二氧化碳腐蚀低合金钢.CN. 101928893 [DB/OL]. 2009-06-23 [ 2010-12-29 ]. http: // search, cnipr. com/search, do? method = detailSearch
18 宝钢,一种抗二氧化碳腐蚀用低合金钢及其制造方法.CN. 101928888 [ DB/OLJ. 2009-06-23 [ 2010-12-29 ]. http: // search, cnipr. com/search, do? method = detailSearch
19 宝钢.一种抗硫化物腐蚀用钢及其制造方法.CN. 101928889 [DB/OL]. 2009-06-23 [ 2010-12-29 ]. http: // search, cnipr. com/ search, do? method = detailSearch
20 宝钢.一种超高强度抗硫化氢腐蚀油井管及其生产方法.CN. 101724785 [ DB/OL]. 2008-10-28 [ 2010-06-09 J. http: // search, cnipr. com/search, do? method = detailSearch
21 宝钢.一种高强度特种抽油杆钢.CN. 101736201 [DB/OLJ. 2009-12-25 [ 2010-06-16 ]. http: // search, cnipr. com/search, do? method = detailSearch
22 宝钢.一种石油套管用钢、电阻焊石油套管及其制造方法.CN. 101921952 [ DB/OLJ. 2009-06-16 [ 2010-12-22 ]. http: // search, cnipr. com/search, do? method = detailSearch
23 宝钢.一种石油套管用钢、电阻焊石油套管及其制造方法.CN. 101845586 [ DB/OLJ. 2009-03-25 [ 2010-09-29 ]. http: H search, cnipr. com/search, do? method = detailSearch
24 宝钢,一种石油套管用钢、高频电阻焊石油套管及其制造方法. CN. 101892422 [ DB/OL ]. 2009-05-19 [ 2010-11-24 ]. http: // search, cnipr. com/search, do? method = detailSearch
25 中石油,直缝电阻焊石油套管用钢及套管制造方法. CN. 101798654 [ DB/OL]. 2010-04-09 [ 2010-08-11 ], http: # search, cnipr. com/search, do? method = detailSearch
26 天津钢管.火烧驱油法开采稠油用油层段石油套管及其生产方 法.CN. 101655002 [ DB/OL]. 2009-09-16 [2010-02-24]. http :〃 search, cnipr. com/search, do? method = detailSearch
27 天津钢管.耐-40 ~ -80 T低温的高强高韧性石油套管-CN. 101629476 [ DB/OLJ. 2009-08-05 [ 2010-01-20 ]. http: // search, cnipr. com/search, do? method = detailSearch
28 天津钢管.屈服强度170 ~ 180ksi钢级的高强高韧性石油套管及 其制造方法.CN. 101892443 [ DB/OL]. 2010-07-09 [2010-11- 24 ]. http: //search, cnipr. com/search, do? method = detailSearch
29 鞍钢.一种高强度直缝焊管用钢及其制造方法.CN. 101906586 [DB/OL]. 2009-06-08 [ 2010-12-08 ]. http: // search, cnipr. com/ search, do? method = detailSearch
30 鞍钢.一种低屈强比直缝电阻焊管用钢及其制造方法.CN. 101818308 [ DB/OLJ. 2009-02-27 [2010-09-01 ]. http: # search, cnipr. com/search, do? method = detailSearch
31 衡阳华菱钢管.稠油热釆井用套管及生产方法.CN. 101871080 [DB/OLJ. 2010-05-26 [ 2010-10-27 ]. http: // search, cnipr. com/ search, do? method = detailSearch
32 攀钢钒钛.3Cr无缝钢管及其制造方法.CN. 101899612 [ DB/ OL]. 2010-07-20[2010-12-01 ]. http: //search, cnipr. com/search, do? method = detailSearch
|