Effect of Carbon Macro-Segregation of Casting Bloom on Banded Structure of Rolled Bar of Gear Steel 20CrMnTiH
Liu Jian1 , Yan Huicheng2, Tang Wei1 , Zhu Wenbing1 , Xu Weiyang2 , Tang Guangbo2
1 Xiangtan Iron and Steel Co Ltd, Hunan Valin, Xiangtan 411101 ;
2 National Engineering Research Center of Continuous Casting Technology, Central Iron and Steel Research Institute, Beijing 100081