Evolution of Inclusions in Stainless Steel 304 during Dephosphorized Hot Metal-110 t AOD-LF-CC-Hot Rolling Process

Chen Chao1, Hou Haibin1 , Cheng Guoguang1 , Pan Jixiang2,Li Yan2 ,Pan Wei2   

  1. 1 State Key Laboratory of Advanced Metallurgy, University of Science and Technology, Beijing 100083 ;
    2 Jiuquan Iron and Steel Group Co, Jiayuguan 735100
  • Received:2012-06-20 Online:2013-02-01 Published:2022-09-14

脱磷铁水410 t AOD-LF-CC-热轧流程304不锈钢中夹杂物的演变

陈超1,侯海滨1,成国光1,潘吉祥2,李岩2,潘伟2   

  1. 1北京科技大学钢铁冶金新技术国家重点实验室,北京100083;
    2酒泉钢铁集团公司,嘉峪关735100
  • 作者简介:陈超(1989-),男,博士研究生,不锈钢精炼和连铸工艺研究。

Abstract: Type, morphology and ingredient of inclusions in stainless steel 304 (/%: 0. 03 ~0. 04C, 0. 39 ~0. 41 Si, L20~1.23Mn, 0. 014 ~0. 016P, 0.001 ~0.002S, 7.95 〜8.00Ni, 18. 06 ~ 18. 20Cr, 0.003 ~ 0. 004Al, 0 〜0.002Ti) during 110 t AOD-LF-tundish-160 mm slab casting-hot rolling strip coil process have been studied by SEM, energy dispersive X-ray spectrometer and analysis by electrolysis. Results show that the 5 ~ 10 μm spheroidal SiO2 -CaO-MgO-Al2 03 type inclusions occur in each steelmaking process, while the 20 μm MnO-Cr2O3 inclusions form in tapping process of AOD, part of which is removed in LF refining process, and they less occur in liquid in tundish and in normal casting slab, but the MnO-Cr2O3 inclusions easily occur in two heats sequence-casting slab, the size of MnO-Cr2O3 inclusion in hot-rolled strip coil is≤5μm. Electrolytic analysis results show that the inclusion amount in two heats sequence-casting slab (4. 65 mg/ 10 kg) increases by 51% as compared with that in normal casting slab (3. 08 mg/10 kg).

摘要: 通过扫描电镜、能谱仪和电解分析研究了在110 t AOD-LF-中间包-160 mm板坯-连铸-热轧板卷生产过程304不锈钢(/%:0.03~0.04C、0.39~0.41Si、1.20~1.23Mn、0.014~0.016P、0.001~0.002S、7.95~8.00Ni、18.06~18.20Cr、0.003~0.004Al、0~0.002Ti)中夹杂物类型、形貌和成分。结果表明,在每一生产阶段都出现5~10μm球形SiO2-CaO-MgO-Al2O3型夹杂,同时在AOD出钢过程产生20μm MnO-Cr2O3型夹杂,LF过程去除一部分MnO-Cr2O3夹杂,中间包和正常浇铸的铸坯中很少出现;但两炉连浇的铸坯易出现MnO-Cr2O3夹杂,热轧板中MnO-Cr2O3夹杂尺寸≤5μm。电解分析结果表明,两炉连浇铸坯中夹杂物数量(4.65 mg/10 kg)比正常浇铸的铸坯(3.08 mg/10 kg)增加了51%。