Numerical Simulation on Flow Field in Vacuum Chamber of 130 t Single Snorkel Furnace with Desulphurizing Top Slag

Rui Qixuan,Cheng Guoguang   

  1. School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083
  • Received:2012-07-15 Online:2013-02-01 Published:2022-09-13

130 t单嘴精炼炉真空室内覆盖脱硫渣的钢液流场数值模拟

芮其宣, 成国光   

  1. 北京科技大学冶金与生态工程学院,北京100083
  • 作者简介:芮其宣( 1975-),男,博士研究生,1997年华东冶金学院(安 徽工业大学)毕业,钢液二次精炼研究:

Abstract: The effect of argon blowing rate (150 ~450 IVmin) and argon blowing location at ladle bottom (ladle center to 3/4 radius of submerged snorkel) on average flow rate at metal-slag interface in 130 t single snorkel furnace with desulphurizing top slag is simulated by Fluent software and VOF model. Results show that the suitable blowing location is at 1/2 radius (R) of submerged snorkel, the average flow rate at metal-slag interface increases with increasing blowing rate, with definite blowing rate and blowing at 1/2R the average flow rate at interface is maximum, and only as blowing location is﹥ 1/2R, the effect of blowing location has obvious effect on variation of slag phase volume fraction at interface.

摘要: 用Fluent软件和VOF模型模拟了130 t单嘴精炼炉内覆盖脱硫渣时钢包底吹氩流量(150~450L/min)和吹氩位置(中心至3/4浸渍管半径)对钢渣界面平均速度的影响。结果表明,吹气位置为1/2浸渍管半径(R)处最合理,钢渣界面平均速度随吹气流量的增加而增加,当流量一定时吹气位置为1/2R时界面平均速度最大;吹气位置﹥1/2R时才会对界面上渣相体积分数变化有显著影响。

关键词: 单嘴精炼炉, 钢渣界面, 流场, 数值模拟;