Analysis on Zinc Balance and Its Control for 1 080 m3 Blast Furnace at Jiyuan Steel

Guo Jiang1 , Li Rong1 , Zhang Fang2   

  1. 1 Dept of Metallurgical and Chemical Engineering, Jiyuan Vocational and Technical College, Jiyuan 454650 ;
    2 Materials and Metallurgy School, Inner Mongolia University of Science and Technology, Baotou 014010
  • Received:2012-12-10 Online:2013-06-01 Published:2022-09-17

济钢1 080 m3高炉锌平衡分析及其控制

郭江1,李荣1,张芳2   

  1. 1济源职业技术学院冶金与化学工程系,济源454650;
    2内蒙古科技大学材料与冶金学院,包头014010
  • 作者简介:郭江(1979-),男,硕士研究生,讲师,2002年包头钢铁学院毕业,高炉炼铁研究。

Abstract: Zinc content in charging and output items for 1 080 m3 No5 blast furnace at Ironmaking Plant, Jiyuan Steel has been analyzed, and combined with real production data of furnace the calculation on equilibrium distribution of zinc is carried out. Results show that zinc load of No5 blast furnace is 625 g/t, in furnace charging, most zinc load is from sinter ore its percentage is up to 72. 22% , next zinc load is from pellet ore it can reach to 24. 13% ; in output items the most amount of zinc is in gas ash which makes up 96. 14% of the total output value. The corresponding measures to control zinc including selecting of charging, optimizing blast furnace operation scheduling and dust de-zincing etc. are presented.

摘要: 测定了济钢炼铁厂5号1 080m3高炉入炉原燃料及产出项的锌含量,并结合高炉实际生产数据进行了锌平衡分布计算。结果表明,5号高炉锌负荷为625g/t,入炉原燃料中,以烧结矿带入的锌最多,可以达到72.22%;其次是球团矿,可以达到24.13%;支出项中,由瓦斯灰带走的锌量最多,占总支出量的96.14%。提出入炉原燃料的选用、高炉操作制度以及含铁尘泥脱锌等相应的控制措施。