Effect of RE on Inclusions and Mechanical Properties of Steel 42CrMoTiB

Si Tingzhi   

  1. School of Materials Science and Engineering, Anhui University of Technology, Ma'anshan 243002
  • Received:2012-12-12 Online:2013-06-01 Published:2022-09-22

稀土对42CrMoTiB钢夹杂物和力学性能的影响

斯庭智   

  1. 安徽工业大学材料科学与工程学院,马鞍山243002
  • 作者简介:斯庭智(1974-),男,博士,副教授,1998年合肥工业大学毕业,新型钢铁材料研究。
  • 基金资助:
    安徽省马鞍山市2011年度市战略性新兴产业科技计划(2011-Z-09)。

Abstract: The test steel 42CrMoTiB and RE microalloying steels 42CrMoTiBRE (/% : 0.41 -0.43C, 0. 36 ~0. 38Si, 0.59~0.72Mn, 0.018 ~ 0.020P, 0.005 ~0.010S, 1.08-1. 13Cr, 0. 16~0. 19Mo, 0. 06 ~ 0.08Ti, 0. 003 ~ 0.004B, 0~ 0. 020Ce or Sm, 0.001 3 ~0.001 5 T [O]) are melted by an 150 kg vacuum induction furnace, casting average cross section 165 mm x 165 mm ingot then forged to 120 mm x 120 mm billet. The effect of Ce or Sm on inclusions and mechanical properties of steel 42CrMoTiB forged billet is studied. Results show that as compared with non-adding RE steel 42CrMoTiB, the inclusion amount in steel 42CrMoTiBRE with adding 0. 18RE ( RE content in steel- 0. 019% ~0. 020% ) decreases obviously ,the inclusion rating units of heavy series A, B and D respectively decrease from 0. 5, 2. 0 and 0. 5 to 0, 0 ~ 0. 5 and 0, and that of thin series respectively decrease from 0. 5, 1. 5 and 2. 0 to 0, 1. 0 and 1. 0; The morphology of inclusions in steel is modified by adding RE to form spherical RE oxysulfide ; and the plasticity and toughness of steel markedly increase by adding RE, as compared with non-adding RE steel 42CrMoTiB the transverse reduction of area (Z) and Charpy V-notch impact energy of steel 42CrMoTiBCe increase respectively from 22% and 17 J/cm2 to 30% and 28 J/cm2.

摘要: 试验42CrMoTiB钢和稀土微合金化42CrMoTiBRE钢(/%:0.41~0.43C、0.36~0.38Si、0.59~0.72Mn、0.018~0.020P、0.005~0.010S、1.08~1.13Cr、0.16~0.19Mo、0.06~0.08Ti、0.003~0.004B、0~0.020Ce或Sm,0.001 3~0.001 5T[O])由150 kg真空感应炉冶炼,浇铸成平均断面尺寸165 mm×165 mm的钢锭,锻成120mm×120 mm钢坯。研究了Ce或Sm对42CrMoTiB钢锻坯夹杂物和力学性能的影响。结果表明,与未加稀土42CrMoTiB钢相比,加入0.18RE后(钢中RE含量0.019%~0.020%)42CrMoTiBRE钢中的夹杂物含量大幅降低,A类、B类和D类粗系夹杂级别分别由0.5、2.0和0.5降低至0、0~0.5和0,细系夹杂分别由0.5、1.5和2.0降低至0、1.0和1.0。加入RE改变了钢中夹杂物形貌,形成球形稀土硫氧化物;加稀土明显提高钢的塑性和韧性,与42CrMoTiB钢相比42CrMoTiBCe钢横向断面收缩率(Z)和夏比冲击功(AKV)分别由22%和17 J/cm2提高至30%和28 J/cm2。 

关键词: 42CrMoTiB钢, 稀土, 夹杂物, 力学性能