Analysis on Process and Technology of Grain Oriented Silicon Steel and Development Trend

Dong Aifeng1 , Zhang Wenkang2   

  1. 1 Technical Center; 2 Silicon Steel Plant, Taiyuan Iron and Steel (Group) Co Ltd, Taiyuan 030003
  • Received:2013-04-22 Online:2013-10-01 Published:2022-09-19

取向硅钢生产工艺技术分析和发展趋势

董爱锋1,张文康2   

  1. 太钢不锈钢股份有限公司1技术中心;2冷轧硅钢厂,太原 030003
  • 作者简介:董爱锋(1976-),女,博士(中科院物理所),髙级工程师,1999年北京科技大学本科毕业,取向硅钢新产品的开发。

Abstract: Main technology parameters of four developed process: cast bloom higher temperature heating-double cold rolling or single cold rolling, lower temperature heating-double cold rolling or single rolling process for production of common grain oriented silicon steel (CGO) and high magnetic induction grain oriented silicon steel (Hi-B) , theory research on grain oriented steel ( Goss nucleus and inhibitor) and present situation of process are summarized in this paper. The development trend of grain oriented silicon steel is increasing (110) [001 ] grain oriented degree, decreasing iron loss of grain oriented silicon steel, developing cast bloom lower temperature heating ( ≤1300 ℃) and thin slab concasting and continuous rolling flow sheet to produce grain oriented silicon steel.

Key words: Grain Oriented Silicon Steel, Casting Bloom Heating, Inhibitor, Secondary Recrystallization, Development Trend

摘要: 介绍了普通取向硅钢(CGO)和高磁感取向硅钢(Hi-B)铸坯高温加热两次冷轧、一次冷轧和铸坯低温加热两次冷轧、一次冷轧法4种成熟生产工艺的主要技术参数,取向硅钢理论研究(Goss晶核和抑制剂)和生产技术现状。取向钢的发展趋势为:提高(110)[001]晶粒取向度,降低取向硅钢铁损,发展铸坯低温加热(≤1300℃)和薄板坯连铸连轧流程生产取向硅钢工艺。

关键词: 取向硅钢, 铸坯加热, 抑制制, 二次再结晶, 发展趋势