Influence of Sizing and Cooling Process on Structure and Mechanical
Properties of N80-1 Seamless Casing Tube of Steel 40Mn2V
Wu Lesheng1, Fang Jian1,2, Li Mingxin1 ,Yuan Zexi2
1 Technical Center, Hengyang Hualing Steel Tube (Group) Co Ltd, Hengyang 421001 ;
2 Key Laboratory for Ferrous
Metallurgy and Resources Utilization of Ministry of Education, Wuhan University of Science and Technology, Wuhan 430081
Wu Lesheng, Fang Jian, Li Mingxin, Yuan Zexi. Influence of Sizing and Cooling Process on Structure and Mechanical
Properties of N80-1 Seamless Casing Tube of Steel 40Mn2V[J]. Special Steel, 2013, 34(6): 45-48.
[1]API 5CT-2005 Specification for Casing and Tubing [S]. American Petroleum Institute Press ,2012,7 : 80-87.
[2]Fang J,Li Y H,Xie K Y,et al. Influence of Hot Deformation on Microstructure of Non-Quenching and Non-Tempering Pipe 36Mn2V Used in Oil Well[A]. ICPNS2010[C] ,China,2010:314.
[3]Fang J,Li Y H,Xie K Y,et al. Study on the Influence of Cooling Rate on the Property of Non-Quenching and Non-Tempering Steel OCTG[J]. Applied Mechanics and Materials,2011,71-78(7) :837- 841.
[4]Fang J,Li Y H,Xie K Y,et al. Influence of Hot Deformation on Microstructure of Non-Quenching and Non-Tempering Pipe 36Mn2V Used in Oil Well [J]. Journal of Materials Science Forum,2011, 704-705(12) :504-509.
[5]方 剑,李阳华,邹喜洋,等.N80级非高质油井管用钢36- 40Mn2V连轧和定径工艺对组织和性能的影响[J].特殊钢, 2012,33(3) :53-56.
[6]方 剑,谢凯意,李阳华,等.V的碳氮化合物析出对36Mn2V非 调质钢组织性能的影响[J].武汉科技大学学报,2012,35(2): 81-84.
[7]刘雅政,刘 照,徐进桥,等.非调质N80石油套管轧制工艺优化的实验研究[J].钢铁,2006,41(7):41-44.
[8] Pan T, Yang C F M. Chemistry and Process Optimization of V-Micro- alloyed N80-Class Seamless Casing Tube [J]. Journal of Iron and Steel Research (International) ,2010,17(3) :72-78.
[9]Liu Z, Liu Y Z,Zhang Y S. Feasibility Experimental Study of New Process of Producting Non-Quenching and Tempering N80 Grad Oil Casings[J]. Hot Working Technology, 2006,35(10) :43-46.
[10]Yan T J ,Wang K H. Effect of Produced Fluid on the Wear Behavior of Grade D Sucker Rod and N80 Type Tubing [J]. Petroleum Science,2005,22(2):116-118.