Effect of Precipitated Phases in New Steel 4Cr3.75MoSiV for
Extrusion Wheel on Thermal Fatigue Behavior
Fei Yang1 , Liu Hongyu1,2, Wang Shengfeng1, Wan Baoyi1, Lin Chong1 , Wang Hongjun1
1 College of Science ;
2 Hubei Province Key Laboratory of Systems Science in Metallurgical
Process, Wuhan University of Science and Technology, Wuhan 430065
Fei Yang, Liu Hongyu, Wang Shengfeng, Wan Baoyi, Lin Chong, Wang Hongjun. Effect of Precipitated Phases in New Steel 4Cr3.75MoSiV for
Extrusion Wheel on Thermal Fatigue Behavior[J]. Special Steel, 2013, 34(6): 49-51.
[1]王颖,樊志新,宋宝韫.TU400型连续挤压机挤压轮温度场测定与模拟[J].有色金属加工,2007,36(4) :42-45.
[2]汪圣锋,刘宏玉,周鹏,等.挤压轮用热作模具钢的研究[J]. 金属热处理,2012,37(7) :98-102.
[3]汪圣锋,刘宏玉.连续挤压包覆机挤压轮用钢的研究进展[J]. 特殊钢,2011,32(1):23-26.
[4]Norstrom L A, Svsson M, Ohrberg N. Thermal Fatigue Behavior of Hot Work Tool Steels[J]. Metals Technology, 1981,8 (10) :376- 381.
[5]宛 农.Mod. 9Cr-1Mo耐热钢中微量元素的作用及控制研究 [D].北京:北京科技大学,1999 :76-79.
[6]Orr J,Burton D. Sensitivity of Microstructure and Mechanical Properties of Steel 91 to Initial Heat Treatments[J], Ironmaking and Steelmaking, 1993,20(6) :415-416.
[7]Robson J D,Bhadeshia H K D H. Modelling Precipitation Sequences in Power Plant Steels, Part1-Kinetic Theory [J]. Materials Science and Technology,1997,13(8) :631 -639.
[8]孙向明,吕松强,张增光.铌、氮、铈对耐热钢性能的影响[J].特殊钢,2002,23(3):16-18.
[9]Tsujii N, Abe G, Fukura K,et al. Effect of Testing Atmosphere on Low Cycle Fatigue of Hot Work Tool Steel at Elevated Temperature [J],ISIJ International, 1995,35(7) :920-926.
[10]曹建春.铌钼复合微合金钢中碳氮化物沉淀析出研究[D].昆 明:昆明理工大学,2006: 102-107.
[11]李健,束德林,郭新成.钨系热作模具钢热疲劳特性的研究 [J].机械工程材料,1988,7(2) :21-31.