ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2014, Vol. 35 ›› Issue (3): 19-23.

Previous Articles     Next Articles

Progress of Research on Interfacial Properties of Fluoride-Containing Slag System for Electroslag Remelting

Cao Yulong , Jiang Zhouhua   

  1. School of Materials and Metallurgy, Northeastern University, Shenyang 110819
  • Received:2013-12-30 Online:2014-06-01 Published:2022-08-27

电渣重熔用含氟渣系界面性质的研究进展

曹玉龙,姜周华   

  1. 东北大学材料与冶金学院,沈阳110819
  • 作者简介:曹玉龙(1990-),男,博士生(东北大学),2012年东北大学 (本科)毕业,电渣冶金技术研究。 姜周华(1963-),男,教授,博士生导师。
  • 基金资助:
    国家自然科学基金资助项目(51274266),
    国家高技术研究发展计划资助项目( 863计划) (N2012AA03A504)。

Abstract: The electroslag remelting (ESR) process of steel mainly occurs in formation period of electrode-end melting drop, and the molten steel is pured and cleaned by slag washing effect as the inclusions in steel are absorbed and solved by slag, while the interfacial tension of slag-steel-inclusion closely affects this process. Based on the research achievements about interfacial properties of fluoride-containing slag system in ESR metallurgy process at home and abroad, the rule of influence of slag ingredient including CaF2, CaO, Al2O3, MgO, Na2O and SiO2 and temperature on molten slag-steel interfacial tension and its internal mechanism are analyzed, while variation rule of the slag-steel interfacial tension with slag ingredient and steel chemical composition, liquid temperature and slag basicity are summarized. To establish experience formula and calculation model of fluoride-containing slag system interfacial property parameters for ESR process is research direction o£ this field.

摘要: 钢的电渣重熔过程主要发生在电极熔化末端熔滴形成阶段,通过渣对钢中夹杂物吸附和溶解的渣洗作用达到提纯和净化钢液的目的,而渣-钢-夹杂物的界面张力密切影响这一过程。本文根据国内外关于电渣重熔过程常用含氟渣系界面性质的研究成果,分析了渣中CaF2、CaO、Al2O3、MgO、Na2O、SiO2等组元及温度对熔渣表面张力的影响规律及内在机理,同时总结了渣-钢界面张力随渣、钢成分及熔体温度、熔渣碱度的变化规律。建立电渣重熔用含氟渣系界面性质参数的经验公式和计算模型是该领域的研究方向。

关键词: 电渣重熔, 含氟渣系, 表面张力, 界面张力, 研究进展