Kong Fanqing, Cheng Xiaojie, Jia Song, Qiao Jianjun, Li Yong , Duan Xiaodong. Development of Chromium-Free Passivating and Finger-Mark
Proofing Hot-Dip Zinc-Coated Steel Sheet[J]. Special Steel, 2014, 35(3): 33-35.
[1]Sakai H, Miki K, Nakamoto T, et al. Development of Thinorganic Composite Coated Steel Sheet With a Fingerprint Re-sistance/ ZINKOBEuA K2-COAT0[J]. Kobel Co Technology Review, 1991, 12(10):58
[2]杨 瓦,潘燕芳.家电用无铬耐指纹热镀锌钢板的研制[J].世界钢铁,2011,13(3):16-17.
[3]文 伟,谭运刚.耐指纹热镀锌板耐蚀性能影响因素分析[C]. 中国钢铁年会论文,2011.
[4]陈义庆,杨志强,徐承明,等.涂镀钢铁产品发展近况[J].鞍钢技术,2006(3):14-18.
[5] Nakamoto T. Complete Chromate-free Production of Electro-galvanized Products at Kobe Steel[R]. R D Kobe Steel Eng-ineering Report,2005,55(2) :3641.
[6]杨兴亮,赵云龙,袁江南.无铬型耐指纹热浸镀锌钢板耐指纹膜对产品属性的影响[J].上海金属,2007,29(5):137-141.
[7]朱文英,译.家电和办公设备用无铬表面处理钢板的开发[J]. 世界钢铁,2006,8(4):14-19.
[8]潘燕芳.武钢热镀锌无铬耐指纹板特性值研究[J],武钢技术, 2008,46(4):33-36.