Composition and Structure of Slag Shell during Electroslag Remelting Process with CaF2-Al2O3-CaO Slag Series

Li Yongbo1, Zhao Junxue1, Tang Wendan1, Dang Yanmei1, Qiu Shengtao2, Cui Yaru1   

  1. 1 School of Metallurgical Engineering, Xi'an University of Architecture and Technology, Xi'an 710055;
    2 National Continuous Casting Center, Central Iron and Steel Research Institute, Beijing 100081
  • Received:2014-02-14 Online:2014-08-01 Published:2022-09-03

CaF2-Al2O3-CaO渣系电渣重熔过程形成的渣皮结构及成分

李永波1, 赵俊学1, 唐雯聃1,党艳梅1,仇圣桃2,崔雅茹1   

  1. 1西安建筑科技大学冶金工程学院,西安710055;
    2钢铁研究总院国家连铸中心,北京100081
  • 作者简介:李永波(1984-),男,硕士研究生,冶金工艺优化与模拟研究。
  • 基金资助:
    国家自然科学资金资助(51174155)

Abstract: The structure and composition of slag shell and final slag during remelting process of 9. 5 t remelting ingot of hot working die steel H13 with 380 kg 60CaF2 -30Al2O3 -10CaO ternary slag system have been analyzed. Results show that during electroslag remelting process the slag shell presents obvious laminating-structure, from out-side to inner-side in proper order being rapid cooling layer, aluminum oxide precipitating layer and inner remelting layer; the CaF2 content in final slag is generally lower than that in initial slag and the CaF2 content in lag shell is higher than that in initial slag; the aluminum oxide content in outside of final slag is highest ; and the oxygen content in remelted slag is obviously higher than that in original slag.

Key words:  , CaF2-Al2O3-CaO Slag Series, Electroslag Remelting(ESR), Slag Shell, Structure

摘要: 分析了9.5 t热作模钢H13重熔锭在380 kg 60CaF2-30Al2O3-10CaO三元渣的重熔过程中渣头和渣皮的结构和成分。结果表明,电渣锭生产过程的渣皮呈现明显的分层结构,自外侧向内,依次为急冷层、氧化铝析出层和内部返熔层;渣头中CaF2含量普遍低于初渣值,而渣皮中CaF2含量高于初渣值;铝氧化物在渣头外缘比重最高;重熔后渣的氧含量明显高于初渣。