Special Steel ›› 2014, Vol. 35 ›› Issue (4): 55-58.

Previous Articles     Next Articles

Effect of Hot Deformation on Structure and Mechanical properties of Quenched and Partitioned Low Carbon CrNi3Si2MoV Steel

Fu Yongtao1,2, Liu Jing1, Wang Cunyu3, Zhang Yujie3,1, Jia Guoxiang3,4, Shi Jie3, Dong Han3   

  1. 1 School of Materials and Metallurgy, Wuhan University of Science and Technology, Wuhan 430080
    2 Research and Development Center, WISCO, Wuhan 430080
    3 Institute for Special Steels, Central Iron and Steel Research Institute, Beijing 100081
    4 School of Metallurgical Engineering, Xi'an University of Architecture and Technology, Xi'an 710055
  • Received:2014-03-03 Online:2014-08-01 Published:2022-09-03

热变形对淬火配分低碳CrNi3Si2MoV钢组织和力学性能的影响

付勇涛1,2, 刘静1, 王存宇3, 张玉杰3,1, 贾国翔3,4, 时捷3, 董瀚3   

  1. 1武汉科技大学材料与冶金学院,武汉430080 ;
    2武汉钢铁集团公司技术研究院,武汉430083;
    3钢铁研究总院特殊钢研究所,北京100081 ;
    4西安建筑科技大学冶金工程学院,西安710055
  • 通讯作者: 通讯作者:刘 静,教授,博士生导师,武汉科技大学材料与冶金学院,武汉430080 E-mail :Eujing@ wust. edu. cn
  • 作者简介:付勇涛(1978-),男,博士生,高级工程师,1999年武汉科技大学(本科)毕业,高强度钢研发。
  • 基金资助:
    青年科学基金项目(51101036),
    国家973项目 (2010CB630803)资助

Abstract: Test steel CrNi3Si2MoV (/% : 0.21C, 1.75Si 0.29Mn, 0.006 0P, 0.0007S, 1.03Cr, 2.86Ni, 0.31 Mo, 0.08V) is melted by a 50 kg vacuum induction furnace and forged to φ15 mm bar product. The effect of hot deformation on structure and hardness of test steel CrNi3Si2MoV austenitized at 1 200 ℃, then hot deforming with 10% 〜 70% at 750 °C + quenching and partitioning (Q&P) treated by quenching to 330 °C and 550 ℃ for 1 min is studied by Gleeble-3800 thermal simulation machine, scanning and transmission electron microscope (SEM and TEM), and X-ray diffractometer (XRD). Test results show that the structure of hot deformation + Q&P treated steel CrNi3Si2MoV is lath martensite + 5. 7% ~ 17.2% lamella residual austenite, with 30% hot deformation the residual austenite amount (17. 2%) in steel is maximum, with 50% hot deformation the hardness HV value of steel is maximum up to 448, and as hot deformation up to 70%, the obvious recrystallization of steel occurs with fine structure and the hardness of steel decreases.

Key words:  , Low Carbon CrNi3Si2MoV Steel, Hot Deformation, Quenching and Partitioning (Q&, P), Martensite, Residual Austenite, Hardness

摘要: 试验用CrNi3Si2MoV钢(/%:0.21C,1.75Si,0.29Mn,0.0060P,0.0007S,1.03Cr,2.86Ni,0.31Mo,0.08V)由50 kg真空感应炉冶炼,并锻成φ15 mm的钢棒。通过Gleeble-3800热模拟试验机、扫描、透射电镜(SEM、TEM)和X-射线衍射仪(XRD)等研究了1 200℃奥氏体化的CrNi3Si2MoV钢在750℃ 10%~70%热变形+淬火至330℃和550℃1 min的淬火分配(Q&P,Qnenching and Partitioning)处理后,热变形量对Q&P处理试验钢组织和硬度的影响。试验结果表明,热变形+Q&P处理后CrNi3Si2MoV钢的组织为板条奥氏体+5.7%~17.2%薄膜状残留奥氏体;变形量为30%时残留奥氏体量最大(17.2%),50%变形时HV值最大为448,当变形量达70%时该钢发生明显的再结晶,组织细化,钢的硬度降低。

关键词: 低碳CrNi3Si2MoV钢, 热变形, Q&, P(淬火分配), 马氏体, 残留奥氏体, 硬度