Numerical Simulation on Effect of Argon Flow Rate on Slag Eye Formation in a 100 t Bottom Blown Ladle
Zhu Lingli1 , Gao Biao1 , Xiang Jie1 , Sun Dongting1 , Tao Huan1 , Zhang Yanli1 , Han Fang2
1. Key Laboratory for Ferrous Metallurgy and Resources Utilization of Ministry of Education,Wuhan University of Science and Technology, Wuhan 430081 ;
2. Wuhan Heavy Industry Casting and Forging Go Ltd, Zhongchuan Heavy Industry, Wuhan 430022;
Zhu Lingli , Gao Biao , Xiang Jie , Sun Dongting , Tao Huan , Zhang Yanli , Han Fang. Numerical Simulation on Effect of Argon Flow Rate on Slag Eye Formation in a 100 t Bottom Blown Ladle[J]. Special Steel, 2014, 35(5): 8-11.
[1] 赵秀清.LF精炼法的发展[J],大型铸锻件,1996,73(3):42-43.
[2] 王立涛,薛正良,张乔英.钢包炉吹氧及夹杂物去除[J].钢铁研究学报,2005,17(3):35-38.
[3] 于新刚,王红卫.迭加法和数值模拟结合分析弹性薄板的优点[J].青岛理工大学报,2006,27(2) :404l.
[4] 郭长庆.带有顶渣的LF钢包炉熔池流动的数学物理模拟研究[J].包头钢学院报,1995,14(3) :27-33.
[5] 成国光,张 鉴.钢包底吹氣搅拌卷渣机理的水模型研究[J]. 钢铁研究学报,1994,2(2) :27-33.
[6] Lage J, Par J. Modeling of Fluid Flow Conditions around the Slag Metal Interface in a Gas-stirred Ladle [J]. ISIJ International, 1996, 36(9):1127-1134.
[7] 曲英,扬健,徐保美.熔渣下金属熔池流动现象数学模拟[J].金属学报,1990,26(3) :157-163.
[8] Iguchi M,Miyamoto M,Yamashita S. Spout Eye Area in Ladle Refi-ning Process[J]. ISIJ International,2004,44(3) :636-638.
[9] 姜钧普,王福明,王新华,等.洁净钢-洁净钢生产工艺技术[M]. 北京:冶金工业出版社,2006,42-43.
[10] 朱苗勇,井本键夫,萧泽强.多孔喷吹钢包内流动和混合过程的 数学物理模拟[J] .金属学报,1995,31(10):435-439.
[11] Yonezawa K, Schwerdtfeger K. Spout Eyes Formed by an Energing Gas Plume at the Surface of a Slag-covered Metal Melt [J]. Metallurgical and Materials Transactions B, 1999,30(3):411 -418.