Application of Induction Heating Liquid in a 30 t Tundish in Continuous Casting Production of Special Steels

Xie Wenxin1,2, Bao Yanping1,2 , Wang Min3 , Zhang Liqiang1,2   

  1. 1 School of Metallurgical and Ecological Engineering,
    2 State Key Laboratory of Advanced Metallurgy,
    3 National Engineering Research Center of Flat Rolling Equipment, University of Science and Technology, Beijing 100083
  • Received:2014-06-12 Online:2014-12-01 Published:2022-08-19

特殊钢连铸生产中30 t中间包感应加热的应用

谢文新1,2,包燕平1,2,王敏3,张立强1,2   

  1. 北京科技大学1冶金与生态工程学院;
    2钢铁冶金新技术国家重点实验室;
    3国家板带生产先进装备工程技术研究中心,北京100083
  • 作者简介:谢文新(1967-),男,博士生(北京科技大学),1989年上海工业大学毕业,特殊钢生产技术。
  • 基金资助:
    博士后科学基金特别资助项目(2013T60062);
    高等学校博士学科点专项科研基金(20130006110023)

Abstract: The 30 t H type tundish Induction heating device is used for production of 370 mm x 490 mm casting bloom of steel grades including bearing steel, steel for tyre cord wire, steel for auto and steel for oil drill tool. The tundish heating principle, equipment structure, masonry technology and heating rating control are presented. Production application results show that the tundish induction heating technology application is available to obviously improve inclusion control level and decrease inclusion index; the superheating extent of liquid decreases from original no-using induction heating technology- 17 ~ 38 ℃ to 8 ~ 25 °C ; the difference between liquid measured superheating extent and aim superheating extent is ± 3 ℃.

摘要: 30t H型中间包感应加热装置用于轴承钢、帘线钢、汽车用钢和石油钻具用钢等钢种的370mm×490mm铸坯的生产。叙述了中间包感应加热原理、设备构成、砌筑和加热档位控制。生产应用结果表明,使用中间包感应加热可明显改善夹杂物控制水平,降低夹杂物指数,钢水过热度从使用前的17~38℃降至8~25℃;钢水实际过热度与目标过热度的差值为±3℃。

关键词: 轴承钢, 汽车用钢, 石油钻具用钢, 30 tH型中间包, 370 mm x 490 mm连铸坯, 感应加热, 夹杂物, 过热度控制