Abstract: The forming process, ingredient and structure of final slag and slag skin during electroslag remelting (ESR) process of 7. 6 t ingot of steel MC5 with 310 kg ANF-6 slag (/% :69.14CaF2,29.51Al2O3,0. 54CaO, 0. 83SiO2) are analyzed and examined. Results show that after ESR the CaF2 and Al2O3 content in final slag decrease obviously and the CaO and SiO2 content increase markedly; the ESR slag skin is divided into three layer from outside to inside of skin, that are the outside-rapid cooling layer, the middle-selective recrystallization layer, in this layer the Al2O3 content is obviously higher than that original value, and the inside third layer-eutectic layer; the average ingredient content in different height has obvious difference, in it the Al2O3 content in median part is obvious higher than original value.
摘要: 分析和检测了MC5钢7.6 t锭总渣量310 kg ANF-6渣系(/%:69.14CaF2,29.51Al2O3,0.54CaO,0.83SiO2)电渣重熔(ESR)过程中渣头、渣皮形成过程、成分和结构。结果表明,ESR后渣中CaF2和Al2O3含量明显降低,CaO、SiO2含量明显增高;ESR渣皮最外层是急冷层,中间层是选分结晶层,Al2O3含量明显高于初始值,第3层是共晶层;渣皮在不同高度的平均成分存在明显差异,其中中部渣皮Al2O3含量明显高于初始值。
关键词: 电渣重熔, ANF-6渣, 渣皮, 成分与组织, Al2O3 选分结晶
Zhao Junxue, Li Yongbo, Zhang Zhenqiang, Li Xiaoming, Cui Yaru , Tang Wendan. Effect of Selective Crystallization of Al2O3 in ANF-6 Slag on Ingredient and Structure of Final Slag and Slag Skin during ESR Process[J]. Special Steel, 2014, 35(6): 9-11.
赵俊学, 李永波, 张振强, 李小明, 崔雅茹, 唐雯聃. 电渣重熔过程ANF-6渣Al2O3选分结晶对渣皮成分和组织的影响[J]. 特殊钢, 2014, 35(6): 9-11.
0 / / Recommend
Add to citation manager EndNote|Ris|BibTeX
URL: https://www.specialsteeljournal.com/EN/
https://www.specialsteeljournal.com/EN/Y2014/V35/I6/9