ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2015, Vol. 36 ›› Issue (3): 23-26.

Previous Articles     Next Articles

Design and Optimization of 180 t Converter Oxygen Lance Nozzle

Liang Huikun, Feng Lianghua, Zhang Ankun , Liu Guanglong   

  1. School of materials and Metallurgy, Liaoning University of Science and Technology, Anshan 114051
  • Received:2014-12-06 Online:2015-06-01 Published:2022-08-17

180 t转炉氧枪喷头的设计和优化

梁慧坤,冯亮花,张安坤,刘广龙   

  1. 辽宁科技大学材料和冶金学院,鞍山114051
  • 通讯作者: 冯亮花
  • 作者简介:梁慧坤(1991-),女,硕士研究生(辽宁科技大学),辽宁科技大学(本科)毕业,氧枪射流模拟。
  • 基金资助:
    国家自然科学基金项目资助(51204093)

Abstract: Based on classical theory for oxygen lance design it is obtained of oxygen lance nozzle with 5 holes for 180 t converter the diameter of inlet 55 mm, the diameter of throat 37. 2 mm, the diameter of outlet 50. 8 mm, the length of contracting section 44. 6 mm, the length of expanding section 97. 2 mm and the length of throat 5 mm ; with using CFD fluid imitation software to simulate the injecting fluid field of oxygen lance with 13°- 17° nozzle at same environmental temperature ,it is obtained for 180 t converter the optimum nozzle angle is 15°its injecting fluid has stronger immersion ability and larger effective impact area.

摘要: 基于氧枪设计的经典理论,得出180 t转炉5孔氧枪喷头的入口直径55 mm,喉口直径37.2 mm,出口直径50.8 mm,收缩段长度44.6 mm,扩张段长度97.2 mm,喉口长度5 mm;采用CFD流体仿真软件模拟在相同环境温度下喷孔夹角13°~17°时氧枪射流流场,得出15°为180 t转炉氧枪最优喷孔夹角,其射流具有较强的穿透能力和较大的有效冲击面积。