Special Steel ›› 2015, Vol. 36 ›› Issue (6): 13-15.
Previous Articles Next Articles
Yang Yongjie
Received:
Online:
Published:
杨咏阶
作者简介:
Abstract: The production flowsheet of ER70S-G welding wire steel containing titanium (/% : 0. 07 C, 0. 82Si, 1. 49Mn, 0. 012P, 0. 010S, 0. 19Ti, 0.0062N) is 80 t top and bottom combined blown converter-LF-150 mm x 150 mm billet casting- coil rolling process. The results of thermodynamic calculation and production practice show that with control of liquid casting temperature ≥1560 °C , [N] ≤78. 6 x 10-6, [Ti/% ] [N/% ] ≤0.00149 and casting speed 2.0 -2.5 m/min, it is available to avoid the precipitation of TiN during casting process and the nozzle clogging.
摘要: ER70S-G含钛焊丝钢(/%:0.07C,0.82Si,1.49Mn,0.012P,0.010S,0.19Ti,0.006 2N)生产流程为80 t顶底复吹转炉-LF-150 mm×150 mm方坯连铸-盘条轧制工艺。热力学计算和生产实践表明,当浇铸温度≥1560℃,[N]≤78.6×10-6,[Ti/%][N/%]≤0.00149及拉速2.0~2.5 m/min时,可以避免在浇铸过程TiN析出和水口结瘤。
关键词: 含钛焊丝钢, TiN, 连铸, 析出, 水口结瘤, 工艺实践
Yang Yongjie. Process Practice to Control of Precipitation of TiN in ER70S-G Welding Wire Steel Containing Titanium and Prevent Nozzle Clogging[J]. Special Steel, 2015, 36(6): 13-15.
杨咏阶. 控制ER70S-G含钛焊丝钢TiN析出和防止水口结瘤的工艺实践[J]. 特殊钢, 2015, 36(6): 13-15.