ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2016, Vol. 37 ›› Issue (2): 19-21.

Previous Articles     Next Articles

Simulation Study on Spread of Thin Strip Rolling by Wire Rod

Li Shengli , Sun Ao , Tian Changjie   

  1. School of Materials and Metallurgy, Liaoning University of Science and Technology, Anshan 114051
  • Received:2015-11-02 Online:2016-04-01 Published:2022-08-06

利用线材轧制薄带宽展的模拟研究

李胜利,孙傲,田长杰   

  1. 辽宁科技大学材料与冶金学院,鞍山 114051
  • 作者简介:李胜利(1967-),男,博士(2006年东北大学),教授,1988年鞍山钢铁学院(本科)毕业,金属压力加工研究。

Abstract: The deformation process of thin strip rolling by hot-rolled rod is simulated and tested by Φ130 mm two-high rolling mill in laboratory using Φ11 mm lead bar to replace hot-rolling rod. Result show that for thickness of thin strip is 1.2 mm the spread can increase by 35.37% by using longitudinal-rolling method, and with increasing the deformation, the change of spread is small; by using diagonal method with decreasing the bite angle the spread increases obviously, the imitate-defined spread formula △b =28.67- 0.26α is obtained, and with bite angle being 20° the width of thin strip is up to 36.12 mm, beside as rolling process is in range of small deformation, with accumulation of reduction the width of rolling piece increases linearly, it is available to get a feasible solution for production of thin-strip with big width-thickness ratio by hot-rolled rod.

Key words: Rod, Diagonal Rolling, Spreading Formula, Thin Strip, Deformation Low

摘要: 在实验室利用Φ11 mm铅棒代替热轧线材,通过Φ130 mm二辊轧机模拟试验热轧圆钢轧制薄带的变形过程。结果表明,当薄带厚度为1.2 mm时,采用纵轧法宽展可增加35.37%,且随着变形量的增多,宽展变化较小;采用角轧法时,随着送入角的减小,宽展增加明显,拟合得到宽展计算公式为△b=28.67-0.26α,当送入角为20°时,薄带宽度可达到36.12 mm。除此之外,在小变形量范围内进行角轧时,轧件的宽度随着压下量的累积呈线性增长,这有利于得到热轧线材生产大宽厚比薄带的可行性解决方案。

关键词: 线材, 角轧, 宽展公式, 薄带, 变形规律