Present Status of Research and Development of Special Seamless Steel Tubes for Oil and Gas Field in Acidic-Corrosive Environment

Xing Na, Huang Bao, He Libo ,Zhao Tingting   

  1. Technology Center, Angang Iron & Steel Co Ltd, Anshan 114009
  • Received:2016-01-28 Online:2016-06-01 Published:2022-08-02

酸性环境用油气专用无缝钢管的研发现状

邢娜,黄宝,何立波,赵婷婷   

  1. 鞍钢股份有限公司技术中心,鞍山H4009
  • 作者简介:邢娜(1984-),女,硕士(2009年东北大学),工程师,2007年辽宁工业大学(本科)毕业,无缝管产品和工艺信息研究。

Abstract: The one of key issue for development of acidic-corrosive oil and gas field is to use H2S stress corrosion cracking resistant seamless steel tube. The research and development of special seamless steel tubes for acidic oil and gas field are carried out at main tube enterprises at home and abroad. The present status of research and development on variety size, grade composition and properties of special seamless steel tubs for oil and gas field in acidic-corrosive environment at Baosteel, Tianjin Steel Tube Co, Hengyang Hualing, Sumitomo Metal, JFE etc enterprises is presented in this article.

摘要: 采用抗H2S应力腐蚀开裂无缝钢管是酸性油气田开发的关键之一。国内外主要钢管企业对酸性油气田专用无缝钢管进行了研究和开发。本文重点介绍了宝钢、天津钢管、衡阳华菱、新日铁住金、JFE等企业酸性环境用油气田专用无缝钢管的品种规格、钢种成分和性能的研发现状。