Dephosphorization Study on 60 t Converter Slagging by Limestone Replacing Lime as Slagging Material

Hao Jiujiu1, Li Hong2, Hu Longfei2,Li Chenxiao2   

  1. 1 Metallurgical Engineering Department, Shanxi Engineering Vocational College, Taiyuan 030009;
    2 Metallurgical and Ecological Engineering School, University of Science and Technology, Beijing 100083
  • Received:2015-12-15 Online:2016-06-01 Published:2022-08-02

60 t转炉石灰石替代石灰造渣脱磷的试验研究

郝赳赳1,李宏2,胡龙飞2,李晨晓2   

  1. 1山西工程职业技术学院冶金工程系,太原030009;
    2北京科技大学冶金与生态工程学院,北京100083
  • 作者简介:郝赳赳(1982-),女,博士(2015年太原理工大学),讲师, 2004年河北理工大学(本科)毕业,钢铁冶金研究。
  • 基金资助:
    国家科技支撑项目资助(2012BAC27B02)

Abstract: The dephosphorizing effect of 60 t converter on 0. 03% ~ 0.27% C, 0. 012% ~ 0. 024% P, 0. 023% ~ 0. 036% S liquid at 1580 ~ 1680 ℃. by limestone replacing lime as slag material is tested and studied to compare the slagsteel phosphor partition ratio by limestone as slagging material with that by lime as slagging material, and to get the effect of TFe in slag, end slag basicity and liquid end temperature by limestone as slag material on slag-steel phosphor partition ratio- Lp. The results show that by limestone replacing lime as slagging material the mode of oxidizing of iron and phosphor in liquid and the dephosphorizing reaction way are same, but the dephosphorizing effect of liquid is better, that is by lime as slagging material the average Lp is 80, while by limestone as slagging material the average Lp is 101. By limestone replacing lime as slagging material the effect of dephosphorizing is best with TFe in slag 14% 〜17% , end slag basicity 3.1〜3. 4 and liquid end temperature 1600 ~1630 ℃.

摘要: 试验研究了60 t转炉采用石灰石替代石灰造渣对0.03%~0.27%C,0.012%~0.024%P,0.023%~0.036%S钢水在1580~1680℃的脱磷效果,对比了石灰石和石灰造渣时渣-钢磷分配比,得出石灰石造渣时渣中TFe,终渣碱度和终点钢水温度对渣-钢磷分配比Lp的影响。结果表明,石灰石替代石灰造渣时,熔池中铁和磷的氧化方式和脱磷反应不变,但钢水的脱磷效果较好:石灰造渣平均Lp为80,石灰石造渣平均Lp为101。石灰石替代石灰造渣炼钢时,渣中TFe含量14%~17%,终渣碱度3.1~3.4,钢水终点温度1600~1630℃时,脱磷效果最好。