Analysis on Characteristics and Exfoliation Mechanism of Oxidized Film at Steam-Side of Steel T91 Tube in Supercritical Power Unit

Liao Shuquan1, Wang Xinmeng2, Tu Yiyou2,Li Guozhong3   

  1. 1 Jiangyin Xingcheng Special Steel Co Ltd, Jiangyin 214429;
    2 School of Materials Science and Engineering, Southeast University, Nanjing 211189 ;
    3 Hubei Xinyegang Steel Co Ltd, Huangshi 435001
  • Received:2015-12-07 Online:2016-06-01 Published:2022-08-04

超临界机组T91钢管蒸汽侧氧化膜特征和脱落机制的分析

廖书全1,王新猛2,涂益友2,李国忠3   

  1. 1江阴兴澄特种钢铁有限公司,江阴214429 ;
    2东南大学材料科学与工程学院,南京211189;
    3湖北新冶钢有限公司,黄石435001
  • 作者简介:廖书全(1973-),男,硕士(2009年北京科技大学),高级工程师,1998年包头钢铁学院毕业,金属材料研究。

Abstract: The ingredient, phases, morphology and exfoliation mechanism of oxide formed at steam-side of Φ90 mm x 10 mm tube of steel T91 (/% : 0. 10C, 0. 35Si, 0. 43Mn, 7. 85Cr, 0. 81 Mo, 0. 24V) for supercritical power unit in vapour at 571. 5 ℃ vapour served for 28800h have been analyzed and studied by optical microscope, scanning electron microscope with energy dispersive spectroscope and X-ray diffractometer. Results show that the thickness of oxide film of steel T91 is about 307. 3 μm with multi-layer structure, its diffusion layer is mixture of Cr2O3 and grains of base metal, the inner oxidized layer is FeCr2O4, the middle oxidized layer is mixture of FeCr2O4 and Fe3O4, and the outer oxidized layer is Fe3O4 and Fe2O3 . There are a lot of pores at FeCr2O4-Fe3O4 interface, by the action of thermal-stress the outer oxidized layer is easily to crack and exfoliate.

摘要: 通过光学显微镜、扫描电镜、能谱仪、X射线衍射仪对超临界机组571.5℃蒸汽服役28 800 h的T91钢(/%:0.10C,0.35Si,0.43Mn,7.85Cr,0.81Mo,0.24V)Φ90 mm×10 mm管材氧化膜的成分、相组成、形貌和脱落机制进行了分析和研究。结果表明,T91钢氧化膜厚度约为307.3μm,呈现多层复杂结构,扩散层为Cr2O3和基体晶粒的混合物,内氧化层为FeCr2O4,中间氧化层为FeCr2O4和Fe2O4的混合物,外氧化层为Fe3O4和Fe2O3。FeCr2O4和Fe3O4的界面处存在大量孔洞,在热应力作用下,外氧化层极易开裂和脱落。