Effect of Activity and Microstructure of Lime on Dephosphorization of Hot Metal

Bo He1 , Dong Jianjun1 , Ren Qianqian2 , Zhang Yuzhu2,3 , Hao Suju3 , Jiang Wufeng3 , Hao Huaqiang2   

  1. 1. Department of Metallurgical Engineering, Tangshan Vocational College of Science and Technology, Tangshan 063000;
    2. School of Metallurgy, Northeastern University, Shenyang 110004;
    3. College of Metallurgy and Energy, North China University of Science and Technology, Tangshan 063009;
  • Received:2016-04-11 Online:2016-10-01 Published:2022-07-28
  • Contact: Hao Suju ,Zhang Yuzhu

石灰活性和微观结构对铁水脱磷的影响

薄荷1,董建君1,任倩倩2,张玉柱2,3,郝素菊3,蒋武锋3,郝华强2   

  1. 1. 唐山科技职业技术学院冶金工程系,唐山 063000;
    2. 东北大学冶金学院,沈阳 110004;
    3. 华北理工大学冶金与能源学院,唐山 063009;
  • 通讯作者: 郝素菊,张玉柱
  • 作者简介:薄荷(1983-),女,硕士(2014年华北理工大学),讲师, 2006年内蒙古科技大学(本科)毕业,炼钢、冶金动力研究。
  • 基金资助:
    国家自然科学基金项目(51174075,51274084);
    河北省自然科学基金项目(E2014209157);

Abstract: The tested hot metal containing 0.40% P is made from commercial iron, phosphoric iron and ferrous sulfide with slagging forming material lime : fluorite =9 :1 and slagging forming material : metal = 1 :50, and melted at 1600℃. by a tube-type electric resistance furnace. The effect of the microstructure of lime-specific surface area (1.05~4.75 m2/ g) , average pore diameter (605~ 404 nm) , pore volume (0.23~0.78 mL/g) and bulk density (0.80~3.10 g/cm3), and the activity of lime (298~350 mL) on dephosphorization of hot metal has been studied by field emission SEM and automatic pressure mercury device. Results show that with increasing the activity of lime the dephosphorization ratio increases gradually ; with increasing the specific surface area, average pore diameter, pore volume and bulk density, the dephosphorization ratio of metal increases first and then decreases ; with lime specific surface area 2.5 m2/g, average pore diameter 750~850 nm, pore volume 0.45 ~0.55 mL/g and bulk density 2.0 g/cm3, the dephosphorization ratio of metal is highest, it is up to 63.0%.

Key words: Lime, Activity, Microscopic Structure, Dephosphorization Rate

摘要: 通过管式电阻炉,用工业铁块、磷铁和硫化亚铁配制0.40%P试验用铁水,造渣剂石灰:萤石=9:1,造渣剂与铁水的比例为1:50,熔融温度1600℃。采用场发射扫描电镜和全自动压汞仪研究了石灰的微观结构-比表面积(1.05~4.75 m2/g)、平均孔径(605~1404 nm)、孔容积(0.23~0.78 mL/g)、体积密度(0.80~3.10 g/cm3)和活性度(298~350 mL)对铁水脱磷的影响。结果表明,随着石灰活性度的增加,铁水脱磷率逐渐增加;随着比表面积、平均孔径、孔容积和体积密度的增加铁水的脱磷率均先增加后降低,当石灰比表面积2.5 m2/g,平均孔径750~850 nm,孔容积0.45~0.55 mL/g,体积密度2.0 g/cm3时铁水的脱磷率达到最好,其铁水脱磷率达到63.0%。

关键词: 石灰, 活性度, 微观结构, 脱磷率